CONTINUOUSLY ORGANIC COATED (COIL COATED) STEEL FLAT PRODUCTS - TECHNICAL DELIVERY CONDITIONS
10-11-2022
05-10-2012
Foreword
1 Scope
2 Normative references
3 Terms and definitions
4 Designation
5 Information to be supplied by the purchaser
6 Requirements
7 Inspection
8 Marking
9 Packing and dispatch
10 Storage
Annex A (informative) - Types of ambience
Annex B (informative) - Coating materials
Annex C (informative) - Types of atmosphere
Annex D (informative) - Outdoor exposure sites
Annex E (informative) - Storage
Bibliography
Explains requirements for continuously organic coated (coil coated) steel flat products.
Committee |
UNSIDER
|
DevelopmentNote |
Supersedes UNI EN 10169-1, UNI EN 10169-2 and UNI EN 10169-3. (11/2010)
|
DocumentType |
Standard
|
PublisherName |
Ente Nazionale Italiano di Unificazione (UNI)
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
Standards | Relationship |
EN 10169:2010+A1:2012 | Identical |
UNI 10372 : 2013 | DISCONTINUOUSLY LAID ROOF COVERINGS - CRITERIA FOR DESIGN, EXECUTION AND MAINTENANCE OF ROOFING MADE OF METAL SHEETS |
UNI 9029 : 2011 | BUILDING - METALLIC PRODUCTS FOR DISCONTINUOUS ROOFING - DESCRIPTIVE CLASSIFICATION |
ISO 9223:2012 | Corrosion of metals and alloys — Corrosivity of atmospheres — Classification, determination and estimation |
EN ISO 4628-2:2016 | Paints and varnishes - Evaluation of degradation of coatings - Designation of quantity and size of defects, and of intensity of uniform changes in appearance - Part 2: Assessment of degree of blistering (ISO 4628-2:2016) |
EN 13523-11:2011 | Coil coated metals - Test methods - Part 11: Resistance to solvents (rubbing test) |
EN 10048:1996 | Hot rolled narrow steel strip - Tolerances on dimensions and shape |
EN 10051:2010 | Continuously hot-rolled strip and plate/sheet cut from wide strip of non-alloy and alloy steels - Tolerances on dimensions and shape |
EN 10140:2006 | Cold rolled narrow steel strip - Tolerances on dimensions and shape |
EN 10079:2007 | Definition of steel products |
EN 13523-12:2017 | Coil coated metals - Test methods - Part 12: Resistance to scratching |
EN 10027-2:2015 | Designation systems for steels - Part 2: Numerical system |
EN 13523-14:2014 | Coil coated metals - Test methods - Part 14: Chalking (Helmen method) |
EN 10152:2017 | Electrolytically zinc coated cold rolled steel flat products for cold forming - Technical delivery conditions |
EN 13523-10:2017 | Coil coated metals - Test methods - Part 10: Resistance to fluorescent UV radiation and water condensation |
EN 13523-26:2014 | Coil coated metals - Test methods - Part 26: Resistance to condensation of water |
EN 13523-6:2002 | Coil coated metals - Test methods - Part 6: Adhesion after indentation (cupping test) |
EN 10268:2006+A1:2013 | Cold rolled steel flat products with high yield strength for cold forming - Technical delivery conditions |
EN 13523-24:2017 | Coil coated metals - Test methods - Part 24: Resistance to blocking and pressure marking |
ISO 2808:2007 | Paints and varnishes Determination of film thickness |
EN ISO 11997-1:2017 | Paints and varnishes - Determination of resistance to cyclic corrosion conditions - Part 1: Wet (salt fog)/dry/humid (ISO 11997-1:2017) |
EN 13523-9:2014 | Coil coated metals - Test methods - Part 9: Resistance to water immersion |
EN 13523-0:2014 | Coil coated metals - Test methods - Part 0: General introduction |
EN 10111:2008 | Continuously hot rolled low carbon steel sheet and strip for cold forming - Technical delivery conditions |
EN 13523-3:2014 | Coil coated metals - Test methods - Part 3: Colour difference - Instrumental comparison |
EN ISO 2409:2013 | Paints and varnishes - Cross-cut test (ISO 2409:2013) |
EN 10346:2015 | Continuously hot-dip coated steel flat products for cold forming - Technical delivery conditions |
EN ISO 9227:2017 | Corrosion tests in artificial atmospheres - Salt spray tests (ISO 9227:2017) |
EN 10139:2016 | Cold rolled uncoated low carbon steel narrow strip for cold forming - Technical delivery conditions |
EN 10025-1:2004 | Hot rolled products of structural steels - Part 1: General technical delivery conditions |
PREN 10338 : DRAFT 2013 | HOT ROLLED AND COLD ROLLED NON-COATED FLAT PRODUCTS OF MULTIPHASE STEELS FOR COLD FORMING - TECHNICAL DELIVERY CONDITIONS |
EN 10088-2:2014 | Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes |
EN 10131:2006 | Cold rolled uncoated and zinc or zinc-nickel electrolytically coated low carbon and high yield strength steel flat products for cold forming - Tolerances on dimensions and shape |
EN ISO 4628-4:2016 | Paints and varnishes - Evaluation of degradation of coatings - Designation of quantity and size of defects, and of intensity of uniform changes in appearance - Part 4: Assessment of degree of cracking (ISO 4628-4:2016) |
EN 13523-21:2017 | Coil coated metals - Test methods - Part 21: Evaluation of outdoor exposed panels |
ISO 4628-4:2016 | Paints and varnishes Evaluation of degradation of coatings Designation of quantity and size of defects, and of intensity of uniform changes in appearance Part 4: Assessment of degree of cracking |
EN 13523-23:2015 | Coil coated metals - Test methods - Part 23: Resistance to humid atmospheres containing sulfur dioxide |
ISO 2810:2004 | Paints and varnishes Natural weathering of coatings Exposure and assessment |
EN ISO 8044:2015 | Corrosion of metals and alloys - Basic terms and definitions (ISO 8044:2015) |
ISO 12944-2:2017 | Paints and varnishes — Corrosion protection of steel structures by protective paint systems — Part 2: Classification of environments |
EN 10143:2006 | Continuously hot-dip coated steel sheet and strip - Tolerances on dimensions and shape |
EN 13523-22:2017 | Coil coated metals - Test methods - Part 22: Colour difference - Visual comparison |
ISO 4628-5:2016 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 5: Assessment of degree of flaking |
EN 10021:2006 | General technical delivery conditions for steel products |
ISO 11997-1:2017 | Paints and varnishes — Determination of resistance to cyclic corrosion conditions — Part 1: Wet (salt fog)/dry/humid |
ISO 8044:2015 | Corrosion of metals and alloys Basic terms and definitions |
EN 13523-18:2002 | Coil coated metals - Test methods - Part 18: Resistance to staining |
EN 13523-27:2017 | Coil coated metals - Test methods - Part 27: Resistance to humid poultice (Cataplasm test) |
EN 10204:2004 | Metallic products - Types of inspection documents |
ISO 2815:2003 | Paints and varnishes Buchholz indentation test |
EN 10088-4:2009 | Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes |
ISO 4997:2015 | Cold-reduced carbon steel sheet of structural quality |
EN 13523-5:2014 | Coil coated metals - Test methods - Part 5: Resistance to rapid deformation (impact test) |
EN 13523-19:2011 | Coil coated metals - Test methods - Part 19: Panel design and method of atmospheric exposure testing |
EN 13523-8:2017 | Coil coated metals - Test methods - Part 8: Resistance to salt spray (fog) |
EN 10130:2006 | Cold rolled low carbon steel flat products for cold forming - Technical delivery conditions |
ISO 4618:2014 | Paints and varnishes — Terms and definitions |
EN 10027-1:2016 | Designation systems for steels - Part 1: Steel names |
EN ISO 2815:2003 | Paints and varnishes - Buchholz indentation test (ISO 2815:2003) |
ISO 9227:2017 | Corrosion tests in artificial atmospheres — Salt spray tests |
EN 13523-7:2014 | Coil coated metals - Test methods - Part 7: Resistance to cracking on bending (T-bend test) |
EN 13523-1:2017 | Coil coated metals - Test methods - Part 1: Film thickness |
EN 13523-25:2014 | Coil coated metals - Test methods - Part 25: Resistance to humidity |
EN ISO 2810:2004 | Paints and varnishes - Natural weathering of coatings - Exposure and assessment (ISO 2810:2004) |
EN 10020:2000 | Definition and classification of grades of steel |
EN 606:2004 | Bar coding - Transport and handling labels for steel products |
EN ISO 4628-5:2016 | Paints and varnishes - Evaluation of degradation of coatings - Designation of quantity and size of defects, and of intensity of uniform changes in appearance - Part 5: Assessment of degree of flaking (ISO 4628-5:2016) |
EN 13523-4:2014 | Coil coated metals - Test methods - Part 4: Pencil hardness |
ISO 2409:2013 | Paints and varnishes Cross-cut test |
EN 13523-15:2015 | Coil coated metals - Test methods - Part 15: Metamerism |
EN 13523-2:2014 | Coil coated metals - Test methods - Part 2: Gloss |
ISO 1043-1:2011 | Plastics — Symbols and abbreviated terms — Part 1: Basic polymers and their special characteristics |
EN ISO 2808:2007 | Paints and varnishes - Determination of film thickness (ISO 2808:2007) |
ISO 4628-2:2016 | Paints and varnishes Evaluation of degradation of coatings Designation of quantity and size of defects, and of intensity of uniform changes in appearance Part 2: Assessment of degree of blistering |
EN ISO 4618:2014 | Paints and varnishes - Terms and definitions (ISO 4618:2014) |
EN 10088-1:2014 | Stainless steels - Part 1: List of stainless steels |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.