THERMAL SPRAYING - MEASUREMENT OF THE ELECTRICAL CONDUCTIVITY OF THERMAL SPRAYED NON-IRON METAL COATINGS BY MEANS OF EDDY CURRENT METHOD
12-08-2014
Foreword
Introduction
1 Scope
2 Normative references
3 Terms and definitions
4 Measuring process
5 Procedure of the measurement
6 Measuring results and their assessment
7 Test report and documentation
Annex A (informative) - Record for the applied
Electrical Conductivity Measurement
Bibliography
Defines the procedure of the measurement of the electrical conductivity of non-Ferro-magnetic thermal sprayed coatings.
Committee |
TC 240
|
DocumentType |
Draft
|
PublisherName |
Comite Europeen de Normalisation
|
Status |
Current
|
Standards | Relationship |
NEN EN 16813 : 2016 | Identical |
DIN EN 16813:2017-02 | Identical |
14/30313326 DC : 0 | Identical |
DIN EN 16813:2015-01 (Draft) | Identical |
NF EN 16813 : 2016 | Identical |
EN ISO 21968:2005 | Non-magnetic metallic coatings on metallic and non-metallic basis materials - Measurement of coating thickness - Phase-sensitive eddy-current method (ISO 21968:2005) |
EN ISO 12718:2008 | Non-destructive testing - Eddy current testing - Vocabulary (ISO 12718:2008) |
EN 2004-1:1993 | Aerospace series - Test methods for aluminium and aluminium alloy products - Part 1: Determination of electrical conductivity of wrought aluminium alloys |
ASTM E 1004 : 2017 : REDLINE | Standard Test Method for Determining Electrical Conductivity Using the Electromagnetic (Eddy Current) Method |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.