NS EN ISO 3506-4 : 2009
Current
The latest, up-to-date edition.
MECHANICAL PROPERTIES OF CORROSION-RESISTANT STAINLESS-STEEL FASTENERS - PART 4: TAPPING SCREWS
01-12-2013
Foreword
Introduction
1 Scope
2 Normative references
3 Designation, marking and finish
3.1 Designation
3.2 Marking
3.3 Finish
4 Chemical composition
5 Mechanical properties and performance
5.1 General
5.2 Mechanical properties
5.3 Thread forming capability
6 Test methods
6.1 Surface hardness test
6.2 Core hardness test
6.3 Torsional strength test
6.4 Drive test
Annex A (informative) Description of groups and grades of
stainless steels
Annex B (informative) Stainless steels for cold heading
and extruding
Annex C (informative) Time-temperature diagram of
intergranular corrosion in austenitic stainless
steels, grade A2 (18/8 steels)
Annex D (informative) Austenitic stainless steels with
particular resistance to chloride-induced
stress corrosion
Annex E (informative) Magnetic properties for austenitic
stainless steels
Bibliography
Describes the mechanical properties of tapping screws made of austenitic, martensitic and ferritic steel grades of corrosion-resistant stainless steels, when tested over an ambient temperature range of 10 degrees C to 35 degrees C.
DocumentType |
Standard
|
PublisherName |
Norwegian Standards (Norges Standardiseringsforbund)
|
Status |
Current
|
Standards | Relationship |
UNI EN ISO 3506-4 : 2010 | Identical |
EN ISO 3506-4:2009 | Identical |
BS EN ISO 3506-4:2009 | Identical |
DIN EN ISO 3506-4:2010-04 | Identical |
ISO 3506-4:2009 | Identical |
UNE-EN ISO 3506-4:2010 | Identical |
I.S. EN ISO 3506-4:2009 | Identical |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.