PLASTICS PIPES FOR THE CONVEYANCE OF FLUIDS UNDER PRESSURE - MINER'S RULE - CALCULATION METHOD FOR CUMULATIVE DAMAGE
Published date
11-23-2012
Publisher
Sorry this product is not available in your region.
Defines a procedure for calculation of the maximum permitted hoop stress applying to pipes exposed to varying internal pressures and/or temperatures during their lifetime. This procedure is called Miner's rule.
Committee |
PRI/88/4
|
DevelopmentNote |
Also numbered as BS EN ISO 13760. (03/2000) Supersedes 96/122205 DC. (01/2006)
|
DocumentType |
Standard
|
PublisherName |
British Standards Institution
|
Status |
Current
|
Supersedes |
Standards | Relationship |
ISO 13760:1998 | Identical |
EN ISO 13760:1998 | Identical |
ISO 12230:2012 | Polybutene-1 (PB-1) pipes — Effect of time and temperature on the expected strength |
ISO 10508:2006 | Plastics piping systems for hot and cold water installations — Guidance for classification and design |
ISO/TR 9080:1992 | Thermoplastics pipes for the transport of fluids — Methods of extrapolation of hydrostatic stress rupture data to determine the long-term hydrostatic strength of thermoplastics pipe materials |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.