ASTM F 2433 : 2005 : R2013
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Test Method for Determining Thermoplastic Pipe Wall Stiffness
Hardcopy , PDF
08-29-2020
English
08-01-2013
CONTAINED IN VOL. 08.04, 2017 Specifies the determination of the load-deflection behavior of thermoplastic pipe wall sections under parallel plate loading conditions.
Committee |
F 17
|
DocumentType |
Test Method
|
Pages |
6
|
ProductNote |
Reconfirmed 2013
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
1.1This test method covers the determination of the load-deflection behavior of thermoplastic pipe wall sections under parallel plate loading conditions.
1.2This test method covers a loading test for determining the wall stiffness of a thermoplastic-pipe wall under a combined load of bending and compression. Changes in pipe wall profile geometry under load may also be determined.
1.3This test method covers thermoplastic pipe.
1.4The characteristics determined by this test method are wall stiffness and changes in profile wall dimensions at specific deformations.
1.5The characteristics determined by this test method are wall stiffness, profile wall efficiency, and for some wall elements stability at specific Strain levels.
1.6The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.
1.7The text of this specification references notes and footnotes that provide explanatory material. These notes and footnotes (excluding those in tables and figures) shall not be considered as requirements of the specification.
1.8This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
ASTM D 618 : 2013 : REDLINE | Standard Practice for Conditioning Plastics for Testing |
AASHTO M 294 : 2015 | SPECIFICATION FOR CORRUGATED POLYETHYLENE PIPE, 300- TO 1500-MM (12- TO 60-IN.) DIAMETER |
AASHTO M 252 : 2009 | SPECIFICATION FOR CORRUGATED POLYETHYLENE DRAINAGE PIPE |
ASTM D 2122 : 2016 : REDLINE | Standard Test Method for Determining Dimensions of Thermoplastic Pipe and Fittings |
ASTM D 695 : 2015 : REDLINE | Standard Test Method for Compressive Properties of Rigid Plastics |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.