ASTM D 3517 : 2014 : REDLINE
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
Standard Specification for “Fiberglass” (Glass-Fiber-Reinforced Thermosetting-Resin) Pressure Pipe
04-25-2020
English
03-01-2014
CONTAINED IN VOL. 08.03, 2017 Specifies machine-made fiberglass pipe, 8 in. (200 mm) through 156 in. (4000 mm), intended for use in water conveyance systems which operate at internal gage pressures of 450 psi (3103 kPa) or less.
Committee |
D 20
|
DevelopmentNote |
Supersedes ASTM D 4163 (02/2003)
|
DocumentType |
Redline
|
Pages |
18
|
PublisherName |
American Society for Testing and Materials
|
Status |
Superseded
|
SupersededBy |
1.1This specification covers machine-made fiberglass pipe, 8 in. (200 mm) through 156 in. (4000 mm), intended for use in water conveyance systems which operate at internal gage pressures of 450 psi (3103 kPa) or less. Both glass-fiber-reinforced thermosetting-resin pipe (RTRP) and glass-fiber-reinforced polymer mortar pipe (RPMP) are fiberglass pipes. The standard is suited primarily for pipes to be installed in buried applications, although it may be used to the extent applicable for other installations such as, but not limited to, jacking, tunnel lining and slip-lining rehabilitation of existing pipelines.
1.2The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are provided for information purposes only.
1.3The following safety hazards caveat pertains only to the test methods portion, Section 8, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
ASTM D 5421 : 2015 : REDLINE | Standard Specification for Contact Molded “Fiberglass” (Glass-Fiber-Reinforced Thermosetting Resin) Flanges |
AWWA M45 : 3 | FIBERGLASS PIPE DESIGN |
FM 1614 : 2017 | FIBER REINFORCED COMPOSITE (FRC) PIPE AND FITTINGS FOR UNDERGROUND FIRE PROTECTION SERVICE |
ASCE/CI 36 15 : 2015 | STANDARD DESIGN AND CONSTRUCTION GUIDELINES FOR MICROTUNNELING |
ASME B31.3:2016 | PROCESS PIPING |
EN ISO 14692-1:2017 | Petroleum and natural gas industries - Glass-reinforced plastics (GRP) piping - Part 1: Vocabulary, symbols, applications and materials (ISO 14692-1:2017) |
ISO 14692-1:2017 | Petroleum and natural gas industries — Glass-reinforced plastics (GRP) piping — Part 1: Vocabulary, symbols, applications and materials |
ANSI/AWWA C950:2013 | FIBERGLASS PRESSURE PIPE |
BS EN ISO 14692-1:2017 | Petroleum and natural gas industries. Glass-reinforced plastics (GRP) piping Vocabulary, symbols, applications and materials |
ASCE 36 01 : 2001 | STANDARD CONSTRUCTION GUIDELINES FOR MICROTUNNELING |
NSF 14 : 2016 | PLASTICS PIPING SYSTEM COMPONENTS AND RELATED MATERIALS |
I.S. EN ISO 14692-1:2017 | PETROLEUM AND NATURAL GAS INDUSTRIES - GLASS-REINFORCED PLASTICS (GRP) PIPING - PART 1: VOCABULARY, SYMBOLS, APPLICATIONS AND MATERIALS (ISO 14692-1:2017) |
ASME B31.3 SPANISH : 2010 | PROCESS PIPING |
NSF 61 : 2016 | DRINKING WATER SYSTEM COMPONENTS - HEALTH EFFECTS |
ASTM D 3859 : 2015 : REDLINE | Standard Test Methods for Selenium in Water |
ISO 1172:1996 | Textile-glass-reinforced plastics — Prepregs, moulding compounds and laminates — Determination of the textile-glass and mineral-filler content — Calcination methods |
ASTM F 477 : 2014 : REDLINE | Standard Specification for Elastomeric Seals (Gaskets) for Joining Plastic Pipe |
ASTM D 790 : 2017 : REDLINE | Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials |
ASTM D 2290 : 2016-12 | TEST METHOD FOR APPARENT HOOP TENSILE STRENGTH OF PLASTIC OR REINFORCED PLASTIC PIPE |
ASTM D 695 : 2015 : REDLINE | Standard Test Method for Compressive Properties of Rigid Plastics |
ASTM D 2992 : 2012 | Standard Practice for Obtaining Hydrostatic or Pressure Design Basis for “Fiberglass” (Glass-Fiber-Reinforced Thermosetting-Resin) Pipe and Fittings |
ASTM D 638 : 2014 : REDLINE | Standard Test Method for Tensile Properties of Plastics |
ASTM D 3892 : 2015 : REDLINE | PRACTICE FOR PACKAGING/PACKING OF PLASTICS |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.