Standard Specification for Steel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service

Available format(s)

Hardcopy , PDF

Superseded date

06-30-2021

Language(s)

English

Published date

09-08-2016

US$66.00
Excluding Tax where applicable

CONTAINED IN VOL. 01.02, 2017 Defines iron base, heat-resisting castings of 25% chromium, 12% nickel class, for structural elements, containers, and supports in electric furnaces, petroleum still tube supports and similar applications up to 2000 degrees F (1095 degrees C).

Committee
A 01
DocumentType
Standard
Pages
4
ProductNote
Reconfirmed 2016
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1This specification covers iron-base, heat-resisting alloy castings of the 25 % chromium, 12 % nickel class, intended for structural elements, containers, and supports in electric furnaces, petroleum still tube supports, and for similar applications up to 2000°F [1095°C].

1.2In the absence of significant proportions of elements other than those prescribed in Section 5, the two types of alloys covered by this specification may in general be distinguished as follows:

1.2.1Type I—Alloys characterized by relatively low limiting creep stress at temperatures between 1500 and 2000°F [815 and 1095°C], and relatively high ductility at ordinary temperatures after aging for short periods at temperatures between 1300 and 1500°F [705 and 815°C].

1.2.2Type II—Alloys having relatively high limiting creep stress but which may develop low ductility at ordinary temperatures when aged for short periods at temperatures between 1350 and 1500°F [730 and 815°C].

1.3The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

1.3.1Within the text, the SI units are shown in brackets.

ASTM A 488/A488M : 2018 : EDT 2 Standard Practice for Steel Castings, Welding, Qualifications of Procedures and Personnel
ASTM A 297/A297M : 2020 Standard Specification for Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant, for General Application
ASTM A 781/A781M : 2020 : REV A Standard Specification for Castings, Steel and Alloy, Common Requirements, for General Industrial Use
ASTM A 957/A957M : 2020 Standard Specification for Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use

ASTM E 8/E8M : 2016 : REV A : EDT 1 Standard Test Methods for Tension Testing of Metallic Materials
ASTM E 8/E8M : 2021 Standard Test Methods for Tension Testing of Metallic Materials
ASTM A 800/A800M : 1991 : R1997 : EDT 1 Standard Practice for Steel Casting, Austenitic Alloy, Estimating Ferrite Content Thereof
ASTM A 957 : 1996 Standard Specification for Investment Castings, Steel and Alloy, Common Requirements, for General Industrial Use
ASTM A 1067 : 2010 Standard Specification for Test Coupons for Steel Castings
ASTM A 800/A800M : 2014 : REDLINE Standard Practice for Steel Casting, Austenitic Alloy, Estimating Ferrite Content Thereof
ASTM E 8/E8M : 2016-09 TEST METHODS FOR TENSION TESTING OF METALLIC MATERIALS

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.