Paints for equipment including ships Solvent-borne - Lead and chromate free - Anticorrosive metal primer
Hardcopy , PDF 1 User , PDF 3 Users , PDF 5 Users , PDF 9 Users
05-03-2018
English
01-01-1994
Specifies requirements for solvent-borne, lead and chromate free, anticorrosive metal primer applied to ships and equipment.
Committee |
CH-003
|
DocumentType |
Standard
|
ISBN |
0 7262 8797 0
|
Pages |
11
|
PublisherName |
Standards Australia
|
Status |
Superseded
|
SupersededBy | |
Supersedes | |
UnderRevision |
This Standard sets out requirements for solvent-borne pigmented metal priming paints for ships and equipment. They are intended to be applied as supplied by brush, roller or spray. The Standard deals with primers that are surface dry within 2 h and may be overcoated after 24 h.This Standard applies to paints intended for the priming of well-cleaned steel or aluminium surfaces, that are to be undercoated with paint specified by AS 4025.2 and then topcoated with a film of semi-gloss enamel to AS 4025.3 or full gloss enamel to AS 4025.1, that will provide resistance to weathering, washing and intermittent contact with petrol or mineral oils. Typical applications include machinery and the superstructures of ships.NOTES:1 Appendix A contains recommendations and advice on information which should be provided by the purchaser at the time of enquiry or order.2 Additional information on the use and application of metal primers is given in Appendix B.
First published as AS 4025.4-1994.
AS 1580.205.1-1981 | Paints and related materials - Methods of test Application properties - Brushing |
AS/NZS 1580.481.1.10:1998 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of flaking and peeling (Reconfirmed 2013) |
AS 1580.481.1.8-1991 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of cracking |
AS 1580.204.1-1990 | Paints and related materials - Methods of test Fineness of grind |
AS 1627.4-2005 | Metal finishing - Preparation and pretreatment of surfaces Abrasive blast cleaning of steel (Reconfirmed 2017) |
AS 1580.452.2-1992 | Paints and related materials - Methods of test resistance to corrosion - Salt droplet test |
AS 1580.214.3-1993 | Paints and related materials - Methods of test Viscosity - Cone-and-plate |
AS/NZS 1580.481.1.6:1998 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of erosion (Reconfirmed 2013) |
AS/NZS 1580.205.3:1997 | Paints and related materials - Methods of test Application properties - Roller coating (Reconfirmed 2013) |
AS 1580.205.3-1981 | Paints and related materials - Methods of test Application properties - Roller coating |
AS 1580.481.1.10-1991 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of flaking and peeling |
AS/NZS 1580.211.2:1995 | Paints and related materials - Methods of test Ease of manual re-incorporation (Reconfirmed 2013) |
AS/NZS 1580.601.1:1995 | Paints and related materials - Methods of test Colour - Visual comparison (Reconfirmed 2013) |
AS 1580.105.2-1993 | Paints and related materials - Methods of test Pretreatment of metal test panels - Sanding |
AS 1580.211.2-1980 | Paints and related materials - Methods of test Ease of manual re-incorporation |
AS/NZS 1580.101.1:1999 | Paints and related materials - Methods of test Conditions of test - Temperature, humidity and airflow control (Reconfirmed 2013) |
AS 1580.104.1-1992 | Paints and related materials - Methods of test Recommended materials for test panels |
AS 1580.601.1-1975 | Paints and related materials - Methods of test Colour - Visual comparison |
AS 2312-1984 | Guide to the protection of iron and steel against exterior atmospheric corrosion |
AS 1627.2-2002 | Metal finishing - Preparation and pretreatment of surfaces Power tool cleaning (Reconfirmed 2017) |
AS/NZS 1580.457.1:1996 | Paints and related materials - Methods of test Resistance to natural weathering (Reconfirmed 2013) |
AS/NZS 1580.481.1.7:1998 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of checking (Reconfirmed 2013) |
AS 2854-1986 | Tinplate cans for general use |
AS 1580.408.4-1993 | Paints and related materials - Methods of test Adhesion (cross-cut) |
AS/NZS 1580.401.1:1999 | Paints and related materials - Methods of test Surface dry condition (Reconfirmed 2013) |
AS/NZS 1580.481.1.9:1998 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of blistering (Reconfirmed 2013) |
AS 1580.452.2-2002 | Paints and related materials - Methods of test Resistance to corrosion - Salt droplet test |
AS 1627.4-1989 | Metal finishing - Preparation and pretreatment of sufaces - Abrasive blast cleaning |
AS 1580.603.1-2002 | Paints and related materials - Methods of test Finish - General appearance (Reconfirmed 2013) |
AS/NZS 1580.403.1:1999 | Paints and related materials - Methods of test Scratch resistance (Reconfirmed 2013) |
AS 1580.401.1-1981 | Paints and related materials - Methods of test Surface dry condition |
AS/NZS 2310:2002 | Glossary of paint and painting terms (Reconfirmed 2016) |
AS 1580.105.1-2002 | Paints and related materials - Methods of test Pretreatment of metal test panels - Solvent cleaning |
AS 1580.203.1-1993 | Paints and related materials - Methods of test Skin formation |
AS 1627.7-1988 | Metal finishing - Preparation and pretreatment of surfaces - Hand tool cleaning of metal surfaces |
AS 4025.3-1993 | Paints for equipment including ships Solvent-borne - Interior and exterior - Semi-gloss enamel |
AS 4025.2-1993 | Paints for equipment including ships Solvent-borne - Interior and exterior - Undercoat |
AS/NZS 1580.202.1:1995 | Paints and related materials - Methods of test Density (Reconfirmed 2013) |
AS 2905-1986 | Steel drums |
AS 1580.105.2-2002 | Paints and related materials - Methods of test Pretreatment of metal test panels - Sanding |
AS 2854-2004 | Tinplate cans for general use |
AS 1580.101.1-1986 | Paints and related materials - Methods of test Air drying conditions |
AS/NZS 1580.101.5:1999 | Paints and related materials - Methods of test Conditions of test - Temperature and humidity control (Reconfirmed 2013) |
AS 2310-1980 | Glossary of paint and painting terms |
AS 4025.1-1992 | Paints for equipment including ships Solvent-borne - Interior and exterior - Full gloss enamel |
AS 1580.214.4-1990 | Paints and related materials - Methods of test - Consistency - Rotothinner |
AS/NZS 1580.481.1.8:1998 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of cracking (Reconfirmed 2013) |
AS 1580.603.1-1992 | Paints and related materials - Methods of test Finish |
AS/NZS 1580.104.1:2000 | Paints and related materials - Methods of test Recommended materials for test panels (Reconfirmed 2013) |
AS 1580.202.1-1980 | Paints and related materials - Methods of test Density |
AS/NZS 1580.205.2:1997 | Paints and related materials - Methods of test Application properties - Conventional spraying (Reconfirmed 2013) |
AS/NZS 1580.204.1:1998 | Paints and related materials - Methods of test Fineness of grind (Reconfirmed 2013) |
AS 1580.401.5-2002 | Paints and related materials - Methods of test Hard dry condition - Sanding test |
AS 1580.301.2-1990 | Paints and related materials - Methods of test Non-volatile content by volume (volume solids) (Reconfirmed 2013) |
AS 1627.2-1989 | Metal finishing - Preparation and pretreatment of surfaces - Power tool cleaning |
AS 1580.457.1-1988 | Paints and related materials - Methods of test Resistance to natural weathering |
AS/NZS 2312:2002 | Guide to the protection of structural steel against atmospheric corrosion by the use of protective coatings |
AS/NZS 1580.214.4:1996 | Paints and related materials - Methods of test Consistency - Rotothinner (Reconfirmed 2013) |
AS/NZS 1580.214.1:1997 | Paints and related materials - Methods of test Consistency - Stormer viscometer (Reconfirmed 2013) |
AS 1580.214.1-1990 | Paints and related materials - Methods of test - Consistency - Stormer viscometer |
AS 1580.481.1.6-1991 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of erosion |
AS 1580.401.5-1993 | Paints and related materials - Methods of test Hard dry condition - Sanding test |
AS 1580.214.3-2003 | Paints and related materials - Methods of test Viscosity - Cone-and-plate |
AS 1580.403.1-1981 | Paints and related materials - Methods of test Scratch resistance |
AS 1580.481.3-2002 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of corrosion of coated metal substrates (Reconfirmed 2013) |
AS 1580.203.1-2004 | Paints and related materials - Methods of test Skin formation |
AS 1580.408.4-2004 | Paints and related materials - Methods of test Adhesion (crosscut) (Reconfirmed 2019) |
AS 1580.103.1-1980 | Paints and related materials - Methods of test Preliminary examination and preparation for testing |
AS 2905-2005 | Steel drums |
AS 1580.211.1-1980 | Paints and related materials - Methods of test Degree of settling |
AS 1580.481.1.9-1991 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of blistering |
AS/NZS 1580.205.1:1997 | Paints and related materials - Methods of test Application properties - Brushing (Reconfirmed 2013) |
AS 1580.105.1-1992 | Paints and related materials - Methods of test Pretreatment of metal test panels - Solvent cleaning |
AS/NZS 1580.205.4:1998 | Paints and related materials - Methods of test Application properties - Airless spraying (Reconfirmed 2013) |
AS 1580.481.3-1992 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of corrosion of coated metal substrates |
AS 1580.205.4-1981 | Paints and related materials - Methods of test Application properties - Airless spraying |
AS 1580.205.2-1981 | Paints and related materials - Methods of test Application properties - Conventional air spraying |
AS/NZS 1580.211.1:1995 | Paints and related materials - Methods of test Degree of settling (Reconfirmed 2013) |
AS 1580.101.5-1986 | Paints and related materials - Methods of test Conditions of test, temperature and humidity controlled |
AS/NZS 1580.103.1:1995 | Paints and related materials Methods of test - Examination and preparation of samples for testing (Reconfirmed 2013) |
AS 1580.481.1.7-1991 | Paints and related materials - Methods of test Coatings - Exposed to weathering - Degree of checking |
AS/NZS 3750.12:1996 | Paints for steel structures Alkyd/micaceous iron oxide (Reconfirmed 2013) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.