1 Scope
2 Normative references
3 Principle
4 Required supplementary information
5 Salt fog test solution
6 Apparatus
7 Sampling
8 Test panels
9 Procedure
10 Examination of test panels
11 Precision
12 Test report
Annex
A Required supplementary information
Defines a test method of determining resistance of coatings to a defined cycle of wet (salt fog)/dry/humidity/UV light conditions using a specified solution.
Committee |
CTN 48
|
DocumentType |
Standard
|
Pages |
16
|
PublisherName |
Asociacion Espanola de Normalizacion
|
Status |
Current
|
Supersedes |
Standards | Relationship |
NF EN ISO 11997-2 : 2013 | Identical |
ISO 11997-2:2013 | Identical |
NBN EN ISO 11997-2 : 2013 | Identical |
NEN EN ISO 11997-2 : 2013 | Identical |
NS EN ISO 11997-2 : 2013 | Identical |
I.S. EN ISO 11997-2:2013 | Identical |
SN EN ISO 11997-2:2013 | Identical |
UNI EN ISO 11997-2 : 2014 | Identical |
BS EN ISO 11997-2:2013 | Identical |
EN ISO 11997-2:2013 | Identical |
DIN EN ISO 11997-2:2013-12 | Identical |
ISO 1514:2016 | Paints and varnishes — Standard panels for testing |
ISO 16474-4:2013 | Paints and varnishes — Methods of exposure to laboratory light sources — Part 4: Open-flame carbon-arc lamps |
ISO 16151:2005 | Corrosion of metals and alloys Accelerated cyclic tests with exposure to acidified salt spray, "dry" and "wet" conditions |
ISO 16474-2:2013 | Paints and varnishes — Methods of exposure to laboratory light sources — Part 2: Xenon-arc lamps |
ISO 2808:2007 | Paints and varnishes Determination of film thickness |
ISO 4628-8:2012 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 8: Assessment of degree of delamination and corrosion around a scribe or other artificial defect |
ISO 11507:2007 | Paints and varnishes Exposure of coatings to artificial weathering Exposure to fluorescent UV lamps and water |
ISO 14993:2001 | Corrosion of metals and alloys Accelerated testing involving cyclic exposure to salt mist, "dry" and "wet" conditions |
ISO 16474-3:2013 | Paints and varnishes Methods of exposure to laboratory light sources Part 3: Fluorescent UV lamps |
ISO 4628-4:2016 | Paints and varnishes Evaluation of degradation of coatings Designation of quantity and size of defects, and of intensity of uniform changes in appearance Part 4: Assessment of degree of cracking |
ISO 15528:2013 | Paints, varnishes and raw materials for paints and varnishes Sampling |
ISO 4628-3:2016 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 3: Assessment of degree of rusting |
ISO 17872:2007 | Paints and varnishes Guidelines for the introduction of scribe marks through coatings on metallic panels for corrosion testing |
ASTM G 152 : 2013 : REDLINE | Standard Practice for Operating Open Flame Carbon Arc Light Apparatus for Exposure of Nonmetallic Materials |
ISO 4628-10:2016 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 10: Assessment of degree of filiform corrosion |
ISO 4628-5:2016 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 5: Assessment of degree of flaking |
ISO 4628-1:2016 | Paints and varnishes Evaluation of degradation of coatings Designation of quantity and size of defects, and of intensity of uniform changes in appearance Part 1: General introduction and designation system |
ISO 4892-3:2016 | Plastics — Methods of exposure to laboratory light sources — Part 3: Fluorescent UV lamps |
ISO 11997-1:2017 | Paints and varnishes — Determination of resistance to cyclic corrosion conditions — Part 1: Wet (salt fog)/dry/humid |
ISO 11341:2004 | Paints and varnishes Artificial weathering and exposure to artificial radiation Exposure to filtered xenon-arc radiation |
ISO 4892-4:2013 | Plastics — Methods of exposure to laboratory light sources — Part 4: Open-flame carbon-arc lamps |
ASTM G 155 : 2013 : REDLINE | Standard Practice for Operating Xenon Arc Light Apparatus for Exposure of Non-Metallic Materials |
ISO 3696:1987 | Water for analytical laboratory use — Specification and test methods |
ISO 9227:2017 | Corrosion tests in artificial atmospheres — Salt spray tests |
ISO 4892-2:2013 | Plastics — Methods of exposure to laboratory light sources — Part 2: Xenon-arc lamps |
ISO 1513:2010 | Paints and varnishes Examination and preparation of test samples |
ISO 4628-6:2011 | Paints and varnishes — Evaluation of degradation of coatings — Designation of quantity and size of defects, and of intensity of uniform changes in appearance — Part 6: Assessment of degree of chalking by tape method |
ISO 3270:1984 | Paints and varnishes and their raw materials — Temperatures and humidities for conditioning and testing |
ISO 4628-2:2016 | Paints and varnishes Evaluation of degradation of coatings Designation of quantity and size of defects, and of intensity of uniform changes in appearance Part 2: Assessment of degree of blistering |
ISO 2135:2017 | Anodizing of aluminium and its alloys — Accelerated test of light fastness of coloured anodic oxidation coatings using artificial light |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.