SAE AMS DTL 22499 : 2013
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
SHIM STOCK, LAMINATED
Hardcopy , PDF
13-05-2018
English
01-01-2013
1. SCOPE
2. APPLICABLE DOCUMENTS
3. REQUIREMENTS
4. VERIFICATION
5. PACKAGING
6. NOTES
Describes the requirements for surface bonded laminated shim stock.
Committee |
AMS-D
|
DevelopmentNote |
Supersedes MIL DTL 22499 (D) (06/2004)
|
DocumentType |
Standard
|
Pages |
11
|
PublisherName |
SAE International
|
Status |
Superseded
|
SupersededBy | |
Supersedes |
Standards | Relationship |
MIL-DTL-22499 Revision D:1998 | Similar to |
SAE AMS 4508 : 2015 | Similar to |
SAE AMS QQ A 250/8 : 2014 | ALUMINUM ALLOY 5052, PLATE AND SHEET |
SAE AMS 5906 : 2006 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 18CR - 9.0NI (SAE 30302), COLD ROLLED, FULL HARD, 185 KSI (1276 MPA) TENSILE STRENGTH |
SAE AMS 5912 : 2014 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 19CR - 9.2NI (SAE 30304), COLD ROLLED, 3/4 HARD, 175 KSI (1207 MPA) TENSILE STRENGTH |
SAE AMS 5903 : 2006 | STEEL, CORROSION-RESISTANT, SHEET, STRIP, AND PLATE, 18CR - 9.0NI (SAE 30302), COLD ROLLED, 1/4 HARD, 125 KSI (862 MPA) TENSILE STRENGTH |
SAE AMS 5905 : 2012 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 18CR - 9.0NI (SAE 30302), COLD ROLLED, 3/4 HARD, 175 KSI (1207 MPA) TENSILE STRENGTH |
SAE AMS 5910 : 2012 | STEEL, CORROSION-RESISTANT, SHEET, STRIP, AND PLATE, 19CR - 9.2NI (SAE 30304) COLD ROLLED, 125 KSI (862 MPA) TENSILE STRENGTH |
SAE AMS 4940 : 2012 | TITANIUM SHEET, STRIP, AND PLATE COMMERCIALLY PURE ANNEALED, 25.0 KSI (172 MPA) YIELD STRENGTH |
SAE AMS 4911 : 2014 | TITANIUM ALLOY, SHEET, STRIP, AND PLATE, 6AL - 4 V, ANNEALED |
SAE AMS 4902 : 2013 | TITANIUM SHEET, STRIP, AND PLATE, COMMERCIALLY-PURE, ANNEALED 40.0 KSI (276 MPA) YIELD STRENGTH |
MIL-I-24768-13 Base Document:1992 | INSULATION, PLASTIC, LAMINATED, THERMOSETTING, COTTON FABRIC BASE, PHENOLIC RESIN (FBE) |
SAE AMS 5913 : 2014 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 19CR - 9.2NI (SAE 30304), COLD ROLLED, FULL HARD, 185 KSI (1276 MPA) TENSILE STRENGTH |
SAE AMS 5513 : 2015 | STEEL, CORROSION-RESISTANT, SHEET, STRIP, AND PLATE, 19CR - 9.2NI (SAE 30304), SOLUTION HEAT TREATED |
SAE AMS 5516 : 2012 | STEEL, CORROSION-RESISTANT, SHEET, STRIP, AND PLATE, 18CR - 9.0NI (SAE 30302), SOLUTION HEAT TREATED |
ASTM B 121/B121M : 2016 : REDLINE | Standard Specification for Leaded Brass Plate, Sheet, Strip, and Rolled Bar |
SAE AMS 5904 : 2012 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 18CR - 9.0NI (SAE 30302), COLD ROLLED, 1/2 HARD, 150 KSI (1034 MPA) TENSILE STRENGTH |
SAE AMS QQ A 250/5 : 2014 | ALUMINUM ALLOY ALCLAD 2024, PLATE AND SHEET |
SAE AMS 5911 : 2014 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 19CR - 9.2NI (SAE 30304) COLD ROLLED, 1/2 HARD, 150 KSI (1034 MPA) TENSILE STRENGTH |
ASTM B 209 : 2014 : REDLINE | Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate |
MIL-I-24768-15 Base Document:1992 | INSULATION, PLASTIC, LAMINATED, THERMOSETTING, COTTON FABRIC BASE, PHENOLIC RESIN (FBI) |
SAE AMS 4901 : 2015 | TITANIUM SHEET, STRIP, AND PLATE, COMMERCIALLY PURE, ANNEALED, 70.0 KSI (485 MPA) |
SAE AMS 4900 : 2014 | TITANIUM SHEET, STRIP, AND PLATE, COMMERCIALLY PURE, ANNEALED, 55.0 KSI (379 MPA) YIELD STRENGTH |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.