SAE AMS 2372 : 2014
Superseded
A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
View Superseded by
QUALITY ASSURANCE SAMPLING AND TESTING, CARBON AND LOW-ALLOY STEEL FORGINGS
Hardcopy , PDF
08-04-2019
English
01-01-2014
1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES
Describes quality assurance sampling and testing procedures used to determine conformance to applicable specification requirements of carbon and low-alloy steel forgings.
Committee |
AMS-E
|
DocumentType |
Standard
|
Pages |
5
|
PublisherName |
SAE International
|
Status |
Superseded
|
SupersededBy |
SAE AMS 6276 : 2016 | STEEL, BARS, FORGINGS, AND TUBING, 0.50CR - 0.55NI - 0.20MO (0.18 - 0.23C) (SAE 8620), CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6263 : 2016 | STEEL BARS, FORGINGS, AND TUBING, 1.2CR - 3.2NI - 0.12MO (0.11 - 0.17C) (9315) |
SAE AMS 5070 : 2016 | STEEL, BARS AND FORGINGS, 0.18 - 0.23C (SAE 1022) |
SAE AMS 6327L : 2017 | STEEL BARS AND FORGINGS, 0.50CR - 0.55NI - 0.25MO (0.38 - 0.43C) (SAE 8740), HEAT TREATED, 125 KSI (862 MPA) TENSILE STRENGTH (COMPOSITION SIMILAR TO UNS G87400) |
SAE AMS 6498 : 2013 | STEEL BARS, FORGINGS, AND TUBING, NITRIDING, 1.4CR - 1.2MO - 0.3V (0.29 - 0.36C), DOUBLE VACUUM MELTED, PREMIUM AIRCRAFT-QUALITY FOR BEARING APPLICATIONS |
SAE AMS 6278 : 2016 | STEEL, BARS, FORGINGS, AND TUBING, 4.1CR - 3.4NI - 4.2MO - 1.2V (0.11 - 0.15C), PREMIUM AIRCRAFT-QUALITY FOR BEARING APPLICATIONS, DOUBLE VACUUM MELTED |
SAE AMS 6409E : 2016 | STEEL, BARS, FORGINGS, AND TUBING 0.80CR - 1.8NI - 0.25MO (0.38 - 0.43C) (SAE 4340) SPECIAL AIRCRAFT QUALITY CLEANLINESS, NORMALIZED AND TEMPERED |
SAE AMS 6304 : 2016 | LOW-ALLOY STEEL, HEAT-RESISTANT, BARS, FORGINGS, AND TUBING, 0.95CR - 0.55MO - 0.30V (0.40 - 0.50C) |
SAE AMS6328N : 2017 | STEEL, BARS, FORGINGS, AND TUBING, 0.50CR - 0.55NI - 0.25MO (0.48 TO 0.53C) (SAE 8750) |
SAE AMS 6411 : 2018 | STEEL BARS, FORGINGS, AND TUBING, 0.88CR - 1.8NI - 0.42MO - 0.08V (0.28 - 0.33C) (4330 MOD) CONSUMABLE ELECTRODE REMELTED |
SAE AMS 6492 : 2013 | STEEL BARS, FORGINGS, AND TUBING, 1.0CR - 3.25NI - 0.40MO (0.17 - 0.22C) AIRCRAFT QUALITY |
SAE AMS 5024 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, FREE-CUTTING, 1.5MN (0.32 - 0.39C) (SAE 1137) |
SAE AMS 6426 : 1990(S2016) | STEEL BARS, FORGINGS, AND TUBING, 0.75SI - 1.0CR - 0.58MO (0.80 - 0.90C), CONSUMABLE ELECTRODE VACUUM MELTED |
SAE AMS 6302K : 2017 | LOW-ALLOY STEEL, HEAT-RESISTANT, BARS, FORGINGS, AND TUBING, 0.65SI - 1.25CR - 0.50MO - 0.25V (0.28 - 0.33C) |
SAE AMS 6443 : 1988 | STEEL BARS, FORGINGS, AND TUBING - 1.0CR (0.98-1.10C) (SAE 51100) CONSUMABLE ELECTRODE VACUUM MELTED |
SAE AMS 6303 : 2018 | STEEL BARS AND FORGINGS, LOW ALLOY, HEAT-RESISTANT, 0.65SI - 1.25CR - 0.50MO - 0.85V (0.25 - 0.30C) |
SAE AMS 6559 : 2013 | STEEL, BARS, WIRE, AND FORGINGS 9.75V - 5.25CR - 1.3MO (2.40 - 2.55C) POWDER METALLURGY PRODUCT HOT ISOSTATICALLY PRESSED |
SAE AMS 6526 : 2016 | STEEL, BARS, FORGINGS, TUBING, AND RINGS, 1.0CR - 7.5NI - 4.5CO - 1.0MO - 0.09V (0.29 - 0.34C), CONSUMABLE ELECTRODE VACUUM REMELTED, ANNEALED |
SAE AMS 6527 : 2018 | STEEL, BARS AND FORGINGS, 2.0CR - 10NI - 14CO - 1.0MO (0.15 - 0.19C), VACUUM MELTED, NORMALIZED AND OVERAGED |
SAE AMS 6299 : 2014 | STEEL BARS, FORGINGS, AND TUBING, CARBURIZING, 0.50CR - 1.8NI - 0.25MO (0.17 - 0.23C) (SAE 4320H) |
SAE AMS 6425 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, 1.4MN - 1.5SI - 0.30CR - 1.8NI - 0.40MO (0.23 - 0.28C), CONSUMABLE ELECTRODE VACUUM MELTED |
SAE MAM 6415 : 1998 | STEEL, BARS, FORGINGS, AND TUBING, 0.80CR - 1.8NI - 0.25MO (0.38 - 0.43C) (SAE 4340) |
SAE AMS 6370 : 2016 | STEEL, BARS, FORGINGS, AND RINGS, 0.95CR - 0.20MO (0.28 - 0.33C) (SAE 4130) |
SAE AMS 6551 : 2013 | STEEL BARS, FORGINGS AND TUBING 1.75CR - 4.0NI - 0.5MO - (0.35 - 0.40C) PREMIUM AIRCRAFT QUALITY CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6499 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, 2.7SI - 0.85CR - 1.8NI - 0.4MO - 0.2V - (0.37 - 0.44C), DOUBLE VACUUM MELTED |
SAE AMS 6322 : 2014 | STEEL BARS, FORGINGS, AND RINGS, 0.50CR - 0.55NI - 0.25MO (0.38 - 0.43C) (SAE 8740) |
SAE AMS 6427 : 2014 | STEEL BARS, FORGINGS, AND TUBING, 0.88CR - 1.8NI - 0.42MO - 0.08V (0.25 - 0.33C) (4330 MOD) |
SAE AMS 6547 : 2013 | STEEL BARS, FORGINGS, AND TUBINGS, 1.0CR - 3.2NI - 0.2MO - (0.12 - 0.17C), AIRCRAFT QUALITY |
SAE AMS 6382 : 2014 | STEEL, BARS, FORGINGS, AND RINGS 0.95CR - 0.20MO (0.38 - 0.43C) (SAE 4140) ANNEALED |
SAE AMS 6447 : 2016 | STEEL, BARS, FORGINGS, AND TUBING, 1.4CR (0.93-1.05C) (SAE 52100), ELECTROSLAG REMELTED |
SAE AMS 6479 : 2015 | STEEL, BARS, FORGINGS, AND TUBING 1.45CR (0.93-1.05C) (SAE 52100) SPECIAL AIRCRAFT-QUALITY CLEANLINESS |
SAE AMS 6432 : 1973 | STEEL BARS, FORGINGS, AND TUBING, 1.05CR - 0.55NI - 1.0MO - 0.12V (0.43-0.49C) |
SAE AMS 6274 : 2016 | STEEL BARS, FORGINGS AND TUBING, 0.50CR - 0.55NI - 0.20MO (0.18 - 0.23C) (SAE 8620) |
SAE AMS 6511 : 2012 | STEEL, MARAGING, BARS, FORGINGS, TUBING, AND RINGS 18NI - 8.5CO - 3.2MO - 0.20TI - 0.10AL DOUBLE VACUUM MELTED, ANNEALED |
SAE AMS 6300 : 2015 | STEEL BARS AND FORGINGS, 0.25MO (0.35 - 0.40C) (SAE 4037) |
SAE AMS 6419 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, 1.6SI - 0.82CR - 1.8NI - 0.40MO - 0.08V (0.40 - 0.45C), CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6494 : 2016 | STEEL BARS, FORGINGS, AND TUBING, 1.0CR - 2.50NI - 2.0MO - 1.10SI (0.10 - 0.20C) AIRCRAFT-QUALITY |
SAE AMS 6417 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, 1.6SI - 0.82CR - 1.8NI - 0.40MO - 0.08V (0.38 - 0.43C), CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6264 : 2014 | STEEL, CARBURIZING GRADE, BARS, FORGINGS, AND TUBING 1.2CR - 3.2NI - 0.12MO (0.14 - 0.20C) (9317) |
SAE AMS 6290 : 2013 | STEEL, BARS AND FORGINGS, CARBURIZING, 1.8NI - 0.25MO (0.11 - 0.17C) (SAE 4615) |
SAE AMS 6422K : 2016 | STEEL, BARS, FORGINGS, AND TUBING, 0.80CR - 0.85NI - 0.20MO - 0.003B - 0.04V (0.38 - 0.43C) (MODIFIED 98BV40) |
SAE AMS 6532 : 2014 | STEEL, BARS AND FORGINGS, 3.1CR - 11.5NI - 13.5CO - 1.2MO (0.21 - 0.25C) VACUUM MELTED, NORMALIZED AND OVERAGED, PRECIPITATION HARDENABLE |
SAE AMS 6558 : 2013 | STEEL, BARS, WIRE, AND FORGINGS 10.5MO - 6W - 3.75CR - 2V (1.25 - 1.40C) POWDER METALLURGY PRODUCT HOT ISOSTATICALLY PRESSED |
SAE AMS 6482 : 2015 | STEEL BARS, FORGINGS, AND TUBING, 1.5SI - 1.25CR - 3.8NI - 0.50MO - 0.30V (0.40C) VACUUM REMELTED, ANNEALED |
SAE AMS 5022 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, FREE-CUTTING, 0.14 - 0.20C (SAE 1117) |
SAE AMS 6470 : 2014 | STEEL, NITRIDING, BARS, FORGINGS, AND TUBING 1.6CR - 0.35MO - 1.13AL (0.38 - 0.43C) (135 MOD) |
SAE AMS 6308 : 2012 | STEEL, BARS AND FORGINGS, 0.90SI - 1.0CR - 2.0NI - 3.2MO - 2.0CU - 0.10V (0.07 - 0.13C), VACUUM ARC OR ELECTROSLAG REMELTED |
SAE AMS 6512 H : 2017 | STEEL, MARAGING, BARS, FORGINGS, TUBING, AND RINGS 18NI - 7.8CO - 4.9MO - 0.40TI - 0.10AL CONSUMABLE ELECTRODE VACUUM MELTED, ANNEALED |
SAE AMS 6493 : 2013 | STEEL BARS, FORGINGS, AND TUBING, 1.0CR - 3.25NI - 0.40MO (0.17 - 0.22C), ELECTROSLAG REMELTED OR CONSUMABLE ELECTRODE VACUUM REMELTED, PREMIUM AIRCRAFT-QUALITY |
SAE AMS 6280 : 2017 | STEEL BARS, FORGINGS, AND RINGS, 0.50CR - 0.55NI - 0.20MO (0.28 - 0.33C) (SAE 8630) |
SAE AMS5062J:2004(S2017) | STEEL, LOW CARBON, BARS, FORGINGS, TUBING, SHEET, STRIP, AND PLATE, 0.25 CARBON, MAXIMUM |
SAE AMS 6320 : 2017 | STEEL BARS, FORGINGS, AND RINGS 0.50CR - 0.55NI - 0.25MO (0.33 - 0.38C) (8735) |
SAE AMS 6484 : 2016 | STEEL, BARS, FORGINGS, AND TUBING 0.80CR - 1.8NI - 0.25MO (0.38 - 0.43C) (SAE 4340) NORMALIZED AND TEMPERED |
SAE AMS 6548 : 2013 | STEEL BARS, FORGINGS, AND TUBING, 1.0CR - 3.2NI - 0.2MO (0.12 - 0.17C), PREMIUM AIRCRAFT-QUALITY, ELECTROSLAG REMELTED OR CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6477 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, 0.80CR (0.90 - 1.03C), FOR BEARING APPLICATIONS |
SAE AMS 6423 : 2016 | STEEL BARS, FORGINGS, AND TUBING, 0.92CR - 0.75NI - 0.52MO - 0.003B - 0.04V (MODIFIED 98BV40) |
SAE AMS 6325 : 2015 | STEEL, BARS, AND FORGINGS 0.50CR - 0.55NI - 0.25MO (0.38 - 0.43C) (SAE 8740) HEAT TREATED, 105 KSI (724 MPA) TENSILE STRENGTH |
SAE AMS 6509A : 2017 | STEEL BARS AND FORGINGS 3.5CR - 7.5NI - 16.3CO - 1.75MO - 0.2W - (0.09 - 0.13C) DOUBLE VACUUM MELTED, NORMALIZED, ANNEALED |
SAE AMS 6539 : 2013 | STEEL BARS, FORGINGS, AND TUBING, 1.7CR - 3.8NI - 0.3MO - (0.32-0.38 C), AIRCRAFT-QUALITY |
SAE AMS 5069 : 2001(S2016) | STEEL BARS, FORGINGS, AND TUBING 0.15 - 0.20C (SAE 1018) |
SAE AMS 6292 : 2014 | STEEL BARS AND FORGINGS, CARBURIZING 1.8NI - 0.25MO (0.15 - 0.20C) (SAE 4617) |
SAE AMS 6324 : 2014 | STEEL BARS, FORGINGS, AND TUBING, 0.65CR - 0.70NI - 0.25MO (0.38 - 0.43C) (8740 MODIFIED) |
SAE AMS 6415 : 2016 | STEEL, BARS, FORGINGS, AND TUBING 0.80CR - 1.8NI - 0.25MO (0.38 - 0.43C) (SAE 4340) |
SAE AMS 6490 : 2014 | STEEL BARS, FORGINGS, AND TUBING 4.0CR - 4.2MO - 1.0V (0.77 - 0.85C) (M-50) PREMIUM AIRCRAFT-QUALITY FOR BEARING APPLICATIONS CONSUMABLE ELECTRODE VACUUM MELTED |
SAE AMS 6414 : 2016 | STEEL, BARS, FORGINGS, AND TUBING 0.80CR - 1.8NI - 0.25MO (0.38 - 0.43C) (SAE 4340) VACUUM CONSUMABLE ELECTRODE REMELTED |
SAE AMS 6517A : 2015 | STEEL, BARS, AND FORGINGS, 3.5CR - 9.5NI - 18CO - 1.1MO (0.13 - 0.17C) DOUBLE VACUUM MELTED, NORMALIZED, ANNEALED |
SAE AMS 6305 : 2016 | STEEL, HEAT-RESISTANT, BARS, FORGINGS, AND TUBING, 0.95CR - 0.55MO - 0.30V (0.40 - 0.50C), VACUUM ARC REMELTED |
SAE AMS 6270 : 2014 | STEEL, BARS, FORGINGS, AND TUBING 0.50CR - 0.55NI - 0.20MO (0.13 - 0.18C) (SAE 8615) |
SAE AMS 6342 K:1990(S2015) | STEEL BARS, FORGINGS, AND TUBING, 0.80CR - 1.0NI - 0.25MO (0.38 - 0.43C) (SAE 9840) |
SAE AMS 6277 : 2016 | STEEL BARS, FORGINGS, AND TUBING, 0.50CR - 0.55NI - 0.20MO (0.18 - 0.23C) (SAE 8620), VACUUM ARC OR ELECTROSLAG REMELTED |
SAE AMS 6267J: 2016 | STEEL BARS, FORGINGS, AND TUBING, 1.2CR - 3.25NI - 0.12MO (0.07 - 0.13C) (9310), ELECTROSLAG REMELTED OR CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6448 : 2013 | STEEL, BARS, FORGINGS AND TUBING 0.95CR - 0.22V (0.48 - 0.53C) (SAE 6150) |
SAE AMS 6444 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, 1.45CR (0.93 - 1.05C) (SAE 52100), PREMIUM AIRCRAFT-QUALITY, CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6497 : 2013 | STEEL BARS, FORGINGS, AND TUBING, NITRIDING 1.4CR - 1.2MO - 0.3V (0.29 - 0.36C), ELECTROSLAG REMELTED OR CONSUMABLE ELECTRODE VACUUM REMELTED, PREMIUM AIRCRAFT-QUALITY FOR BEARING APPLICATIONS |
SAE AMS 6340 : 2014 | STEEL BARS, FORGINGS, AND TUBING 0.88CR - 1.8NI - 0.42MO - 0.08V (0.28 - 0.33C) (4330 MOD) CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6255F : 2016 | STEEL BARS, FORGINGS, AND TUBING, 1.1SI - 1.45CR - 1.0MO - 0.08AL (0.16 - 0.22C), DOUBLE VACUUM MELTED |
SAE AMS 6478 : 2001 | STEEL, BARS AND FORGINGS - 3.1CR - 11.5NI - 13.5CO - 1.2MO (0.21 - 0.25C) VACUUM MELTED, ANNEALED HEAT TREATABLE TO 290 KSI (1999 MPA) TENSILE STRENGTH |
SAE AMS 6429 : 2014 | STEEL BARS, FORGINGS, TUBING, AND RINGS 0.78CR - 1.8NI - 0.35MO - 0.20V (0.33 - 0.38C) (4335 MOD) CONSUMABLE ELECTRODE VACUUM MELTED |
SAE AMS 6412 : 2015 | STEEL, BARS AND FORGINGS 0.80CR - 1.8NI - 0.25MO (0.35 - 0.40C) (4337) |
SAE AMS 6294 : 2014 | STEEL BARS AND FORGINGS, CARBURIZING 1.8NI - 0.25MO (0.17 - 0.22C) (SAE 4620) |
SAE AMS 6260S : 2016 | STEEL, BARS, FORGINGS, AND TUBING, 1.2CR - 3.2NI - 0.12MO (0.07 - 0.13C) (9310) |
SAE AMS 6549 : 2013 | STEEL BARS, FORGINGS, AND TUBING, 1.0CR - 3.2NI - 0.2MO (0.12 - 0.17C), PREMIUM AIRCRAFT-QUALITY, DOUBLE VACUUM MELTED |
SAE AMS 6408 : 2018 | STEEL, HOTWORK TOOL, BARS AND FORGINGS, 5.25CR - 1.5MO - 1.0V (0.35-0.45C) (H-13), ELECTROSLAG REMELTED (ESR) OR CONSUMABLE ELECTRODE VACUUM ARC REMELTED (VAR), ANNEALED |
SAE AMS 6496 : 2013 | STEEL BARS, FORGINGS, AND TUBING, NITRIDING, 1.4CR - 1.2MO - 0.3V (0.29 - 0.36C) AIRCRAFT-QUALITY FOR BEARING APPLICATIONS |
SAE AMS 6272 : 2014 | STEEL BARS, FORGINGS, AND TUBING 0.50CR - 0.55NI - 0.20MO (0.15 - 0.20C) (SAE 8617) |
SAE AMS 6312 : 2015 | STEEL BARS, FORGINGS, AND TUBING, 1.8NI - 0.25MO (0.38 - 0.43C) (4640) |
SAE AMS 6519 : 2014 | STEEL, MARAGING, BARS, FORGINGS, TUBING, AND RINGS 19NI - 3.0MO - 1.4TI - 0.10AL PREMIUM AIRCRAFT QUALITY DOUBLE VACUUM MELTED, ANNEALED |
SAE AMS 6516 : 2017 | STEEL, BARS AND FORGINGS 1CR - 10NI - 7CO - 2MO - 1.3W - 0.1V - (0.28 - 0.32C) VACUUM INDUCTION MELTED, VACUUM ARC REMELTED, NORMALIZED AND ANNEALED PRECIPITATION HARDENABLE |
SAE AMS 6250 : 2015 | STEEL BARS, FORGINGS, AND TUBING, 1.5CR - 3.5NI (0.07 - 0.13C) (3310) |
SAE AMS 6557 : 2013 | STEEL, BARS, WIRE, AND FORGINGS, 9V - 5.25CR - 1.3MO (1.80 - 1.95C), POWDER METALLURGY PRODUCT, HOT ISOSTATICALLY PRESSED |
SAE AMS 6543 : 2016 | STEEL, BARS AND FORGINGS, 2.0CR - 10NI - 8.0CO - 1.0MO (0.10 - 0.14C) (HY-180), DOUBLE VACUUM MELTED, SOLUTION HEAT TREATED, MARAGE HARDENABLE |
SAE AMS 6424 : 2017 | STEEL BARS, FORGINGS, AND TUBING 0.80CR - 1.8NI - 0.25MO (0.49 - 0.55C) |
SAE AMS 6560 : 2013 | STEEL BARS, WIRE AND FORGINGS 10CO - 7MO - 6V - 6W - 4CR (2.2 - 2.4C) PREMIUM AIRCRAFT-QUALITY FOR BEARING APPLICATIONS INERT GAS ATOMIZED AND HOT ISOSTATICALLY PRESSED CONSOLIDATED |
SAE AMS6481D:2017 | STEEL BARS, FORGINGS, AND TUBING, NITRIDING, 3CR - 1MO - 0.2V - (0.29 - 0.36C), PREMIUM AIRCRAFT-QUALITY FOR BEARING APPLICATIONS, DOUBLE VACUUM MELTED |
SAE AMS 6421 : 2016 | STEEL BARS, FORGINGS, AND TUBING 0.80CR - 0.85NI - 0.20MO - 0.003B (0.35 - 0.40C) (MODIFIED 98B37) |
SAE AMS 5060 : 2003(S2016) | STEEL, BARS, FORGINGS AND TUBING 0.13 - 0.18C (SAE 1015) |
SAE AMS 5080 : 2016 | STEEL, BARS, FORGINGS, AND TUBING, 0.31 - 0.38C (SAE 1035) |
SAE AMS6475K | STEEL, NITRIDING, BARS, FORGINGS, AND TUBING, 1.1CR - 3.5NI - 0.25MO - 1.2AL (0.21 - 0.26C) |
SAE AMS 6430J : 2017 | STEEL, BARS, FORGINGS, TUBING, AND RINGS, 0.75MN - 0.78CR - 1.8NI - 0.35MO - 0.20V (0.32 - 0.38C), (4335 MODIFIED) |
SAE AMS 6515 : 2012 | STEEL, MARAGING, BARS, FORGINGS, TUBING, AND RINGS 18.5NI - 12.0CO - 4.9MO - 1.40TI - 0.10AL DOUBLE VACUUM MELTED, ANNEALED |
SAE MAM 6304 : 1994 | LOW-ALLOY STEEL, HEAT-RESISTANT, BARS, FORGINGS, AND TUBING, 0.95CR - 0.55MO - 0.30V (0.40 - 0.50C) |
SAE AMS 6495 : 2016 | STEEL BARS, FORGINGS, AND TUBING, 1.0CR - 2.50NI - 2.0MO - 1.10SI (0.10 - 0.20C), PREMIUM AIRCRAFT-QUALITY, ELECTROSLAG REMELTED OR CONSUMABLE ELECTRODE VACUUM REMELTED |
SAE AMS 6407 : 2017 | STEEL, BARS, FORGINGS, AND TUBING, 1.2CR - 2.0NI - 0.45MO (0.27 - 0.33C) |
SAE AMS 6317K : 2017 | STEEL BARS AND FORGINGS, 1.8NI - 0.25MO (0.38 - 0.43C) (4640), HEAT TREATED, 125 KSI (862 MPA) TENSILE STRENGTH |
SAE AMS 6431 : 2017 | STEEL, BARS, FORGINGS, AND TUBING, 1.05CR - 0.55NI - 1.0MO - 0.11V (0.45 - 0.50C) (D6AC), VACUUM CONSUMABLE ELECTRODE REMELTED |
SAE AMS 6487 : 2016 | STEEL, BARS, AND FORGINGS, 5.0CR - 1.3MO - 0.50V (0.38 - 0.43C) (H-11), CONSUMABLE ELECTRODE VACUUM MELTED |
SAE AMS 6514 : 2017 | STEEL, MARAGING, BARS, FORGINGS, TUBING, AND RINGS 18.5NI - 9.0CO - 4.9MO - 0.65TI - 0.10AL CONSUMABLE ELECTRODE VACUUM MELTED, ANNEALED |
SAE AMS 2370 : 2016 | QUALITY ASSURANCE SAMPLING AND TESTING, CARBON AND LOW-ALLOY STEEL WROUGHT PRODUCTS AND FORGING STOCK |
SAE AMS 6265 : 2016 | STEEL, BARS, FORGINGS, AND TUBING, 1.2CR - 3.25NI - 0.12MO (0.07 - 0.13C) (9310), VACUUM CONSUMABLE ELECTRODE REMELTED |
SAE AMS 6442 : 1987 | STEEL BARS AND FORGINGS 0.50Cr (0.98-1.10C) (SAE 50100) FOR BEARING APPLICATIONS |
SAE AMS 6440 : 2015 | STEEL, BARS, FORGINGS, AND TUBING, 1.45CR (0.93 - 1.05C) (SAE 52100), FOR BEARING APPLICATIONS |
SAE AMS6491E | STEEL BARS, FORGINGS, AND TUBING 4.1CR - 4.2MO - 1.0V (0.80 - 0.85C) (M-50) PREMIUM AIRCRAFT-QUALITY FOR BEARING APPLICATIONS, DOUBLE VACUUM MELTED |
SAE AMS 6525 : 2016 | STEEL, BARS, FORGINGS, TUBING, AND RINGS, 0.75CR - 9.0NI - 4.5CO - 1.0MO - 0.09V (0.17 - 0.23C), CONSUMABLE ELECTRODE VACUUM MELTED |
SAE AMS 6330 : 2017 | STEEL BARS, FORGINGS, AND TUBING, 0.65CR - 1.25NI (0.33 - 0.38C) |
SAE AMS 6471 : 2014 | STEEL, NITRIDING, BARS, FORGINGS, AND TUBING 1.6CR - 0.35MO - 1.13AL (0.38 - 0.43C) (135 MOD) CONSUMABLE ELECTRODE VACUUM MELTED |
SAE AMS 6556 : 2013 | STEEL, BARS, WIRE, AND FORGINGS, 8V - 4CR - 4W - 3MO (2.45 - 2.55C), POWDER METALLURGY PRODUCT, HOT ISOSTATICALLY PRESSED |
SAE AMS 6257 : 2016 | STEEL BARS, FORGINGS, AND TUBING, 1.6SI - 0.82CR - 1.8NI - 0.40MO - 0.08V (0.40 - 0.44C), CONSUMABLE ELECTRODE VACUUM REMELTED, NORMALIZED AND TEMPERED |
SAE AMS 6428 : 2014 | STEEL, BARS, FORGINGS, AND TUBING 0.78CR - 1.8NI - 0.35MO - 0.20V (0.32 - 0.38C) (4335 MOD) |
SAE AMS 6472 : 2014 | STEEL, BARS AND FORGINGS, NITRIDING 1.6CR - 0.35MO - 1.1AL (0.38 - 0.43C) (135 MOD) HARDENED AND TEMPERED, 112 KSI (772 MPA) TENSILE STRENGTH |
SAE AMS 2808 : 2017 | IDENTIFICATION FORGINGS |
ASTM E 8/E8M : 2016-09 | TEST METHODS FOR TENSION TESTING OF METALLIC MATERIALS |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.