DEFSTAN 05-50(PT29)/1(1986) : 1986
Current
The latest, up-to-date edition.
METHODS FOR TESTING FUELS, LUBRICANTS AND ASSOCIATED PRODUCTS - PART 29: CORROSIVENESS AND OXIDATION STABILITY OF OILS AND HYDRAULIC FLUIDS
Hardcopy , PDF
English
18-07-1986
Preface
0 Introduction
1 Scope
2 Warning
3 Related Documents
4 Outline of Method
5 Apparatus
6 Materials
7 Preparation of Apparatus
8 Procedure
9 Calculation
10 Reporting
11 Precision
Determines corrosiveness and oxidation stability of hydraulic fluids and oils.
DevelopmentNote |
Supersedes DEFSTAN 05-50/1(1979) (05/2003)
|
DocumentType |
Standard
|
Pages |
16
|
PublisherName |
UK Ministry of Defence Standards
|
Status |
Current
|
Supersedes |
DEFSTAN 91-47/1(1980) : 1980 | LUBRICATING OIL, GENERAL PURPOSE: LOW TEMPERATURE NATO CODE NO. O-142 JOINT SERVICE DESIGNATION: OM-12 |
DEFSTAN 91-71/2(2001) : 2001 | LUBRICATING OIL, GEAR SYNTHETIC JOINT SERVICE DESIGNATION: OX-165 |
DEFSTAN 80-34/3(1995) : 1995 | CORROSION PREVENTIVE, OIL, THIN FILM JOINT SERVICE DESIGNATION: PX-4 |
DEFSTAN 91-102/2(2000) : 2000 | LUBRICATING OIL, CORROSION PREVENTIVE, SMALL ARMS AND LIGHT CALIBER WEAPONS NATO CODE: O-157 JOINT SERVICE DESIGNATION: OX-24 |
DEFSTAN 91-102/1(1995) : INTERIM | LUBRICATING OIL, CORROSION PREVENTIVE, SMALL ARMS AND LIGHT CALIBRE WEAPONS NATO CODE: 0-157 JOINT SERVICE DESIGNATION: OX-24 |
DEFSTAN 91-71/1(1989) : 1989 | LUBRICATING FLUID, GEAR, SYNTHETIC JOINT SERVICE DESIGNATION: OX-165 |
DEFSTAN 91-48/2(1997) : 1997 | HYDRAULIC FLUID, PETROLEUM: SUPERCLEAN NATO CODE: H-515 JOINT SERVICE DESIGNATION: OM-15 HYDRAULIC FLUID, PETROLEUM: NORMAL NATO CODE: H-520 JOINT SERVICE DESIGNATION: OM-18 |
DEFSTAN 80-142/2(2002) : 2002 | CORROSION PREVENTIVE: HYDRAULIC SYSTEM NATO CODE: C-635 JOINT SERVICE DESIGNATION: PX-26 |
DEFSTAN 91-49/1(1980) : 1980 | LUBRICATING OIL, INSTRUMENT: SYNTHETIC NATO CODE NO. O-147 JOINT SERVICE DESIGNATION: OX-14 |
IP 71 : 1995 | SECTION 1: PETROLEUM PRODUCTS - TRANSPARENT AND OPAQUE LIQUIDS - DETERMINATION OF KINEMATIC VISCOSITY AND CALCULATION OF DYNAMIC VISCOSITY - SECTION 2: GLASS CAPILLARY KINEMATIC VISCOMETERS - SPECIFICATIONS AND OPERATING INSTRUCTIONS (TWO PART SET) |
DEFSTAN 03-4/4(1998) : 1998 | THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA |
BS 2000-154(1999) : 1999 | PETROLEUM PRODUCTS - CORROSIVENESS TO COPPER - COPPER STRIP TEST |
BS 3370:1970 | Specification for wrought magnesium alloys for general engineering purposes. Plate, sheet and strip |
BS 2000-71(1990) : 1990 | METHODS OF TEST FOR PETROLEUM AND ITS PRODUCTS - KINEMATIC VISCOSITY OF TRANSPARENT AND OPAQUE LIQUIDS AND CALCULATION OF DYNAMIC VISCOSITY |
BS L 156:1978 | Specification for sheet and strip of aluminium-copper-magnesium-silicon-manganese alloy (solution treated and aged at room temperature) (Cu 4.4, Mg 0.5, Si 0.8, Mn 0.8) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.