Foreword
Introduction
1 Scope
2 Warning
3 Normative References
4 Definitions
4.2 Process Control Schedule
4.3 Significant Surface
4.4 Tensile Strength of Steels
4.4.1 Tensile Strength
4.4.2 Tensile strength/hardness relationship
5 Information to be Supplied to the Processor
6 Process Control
7 Preparation for Coating
8 Reclamation of Worn or Over-Machined Items
9 Condition of Substrate (Process Requirements)
10 Minimising the Risk of Hydrogen Embrittlement of Steel Items
11 Stress Relief
12 Introduction to Surface Compressive Stresses
12.1 Shot Peening
12.2 Other methods
13 Preparation for Plating
13.1 General Requirements
13.2 Cleaning
14 Electro-Deposition of Nickel
15 Post Plating Heat Treatment
15.1 Steel
15.2 Aluminium and aluminium alloys
16 Inspection, Sampling and Testing
16.1 General
16.2 Inspection
16.3 Thickness
16.4 Adhesion
16.5 Hardness
17 Treatment of Items Rejected During Inspection and Test
Annex A - Nickel Plating Solutions and Conditions
A.1 Process 1
A.2 Process 2
A.3 Process 3
A.4 Process 4
A.5 Process 5
Annex B - The Analysis of Nickel Plating Solutions
B.1 General requirements
B.2 Determination of Nickel
B.2.1 Methodology
B.2.2 Principle
B.2.3 Reagents
B.2.4 Special Apparatus
B.2.5 Procedure
B.2.6 Expression of results - Methods of calculation
B.3 Determination of chloride
B.3.1 Methodology
B.3.2 Principle
B.3.3 Reagents
B.3.4 Procedure
B.3.5 Expression of results
B.4 Determination of ammonium
B.4.1 Methodology
B.4.2 Principle
B.4.3 Reagents
B.4.4 Special apparatus
B.4.5 Procedure
B.4.6 Expression of results - Methods of calculation
B.5 Determination of total nitrogen
B.5.1 Methodology
B.5.2 Principle
B.5.3 Reagents
B.5.4 Special apparatus
B.5.5 Procedure
B.5.6 Expression of results - Methods of calculation
B.6 Determination of Boric Acid
B.6.1 Methodology
B.6.2 Principle
B.6.3 Reagents
B.6.4 Special apparatus
B.6.5 Procedure
B.6.6 Expression of results - Methods of calculation
Annex C - Additional Requirements and Information
C.1 General
C.1.1 Deposit Hardness
C.1.2 Galling
C.1.3 Fatigue strength
C.1.4 Spring steel
C.2 Preparation for Plating
C.3 Nickel Plating Solution
C.4 Deposition
C.5 Rinsing
Annex D - Adhesion Tests
D.1 Adhesle Test
D.2 Burnishing Test
D.3 File Test
D.4 Quenching Test
Annex E - Chemical Methods of Stripping Nickel Deposits
E.1 Nickel (and Copper) on Aluminium
E.2 Nickel Copper
E.3 Nickel on Steel
E.4 Proprietary Solutions
Specifies the requirements for the nickel-plating of ferrous metals, copper alloys, aluminium alloys and zinc alloys for one or more of the following purposes: (a) the production of wear-resistant surfaces; (b) the building up of worn or over-machined surfaces; (c) corrosion resistance; (d) to provide an undercoat for subsequent deposits, e.g. chromium.
DevelopmentNote |
Supersedes DEFSTAN 03-27/2(1998) (10/2005) This standard is obsolescent because it is no longer required for the procurement of new equipment but is retained for maintenance purposes in support of existing in-service equipment. (05/2013)
|
DocumentType |
Standard
|
Pages |
34
|
PublisherName |
UK Ministry of Defence Standards
|
Status |
Withdrawn
|
SupersededBy | |
Supersedes |
SAE AMS03-4A : 2015(S2017) | THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA |
SAE AMS 03-14 : 2018 | ELECTRODEPOSITION OF CHROMIUM FOR ENGINEERING PURPOSES |
DEFSTAN 03-4/5(2006) : 2006 | THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA |
DEFSTAN 03-2/6(2011) : 2011 | CLEANING AND PREPARATION OF METAL SURFACES |
DEFSTAN 03-36/2(2010) : 2010 | GUIDANCE TO THE USE OF CADMIUM ALTERNATIVES IN THE PROTECTIVE COATING OF DEFENCE EQUIPMENT |
DEFSTAN 03-2/5(2009) : 2009 | CLEANING AND PREPARATION OF METAL SURFACES |
DEFSTAN 03-4/6(2011) : 2011 | THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA |
SAE AMS 03-2 : 2017 | CLEANING AND PREPARATION OF METAL SURFACES |
BS 6200-3.22.1:1992 | Sampling and analysis of iron, steel and other ferrous metals. Methods of analysis. Determination of nitrogen Steel: volumetric method |
BS 1752:1983 | Specification for laboratory sintered or fritted filters including porosity grading |
BS EN ISO 3696:1995 | Water for analytical laboratory use. Specification and test methods |
BS EN ISO 6507-1:2005 | Metallic materials. Vickers hardness test Test method |
DEFSTAN 03-4/4(1998) : 1998 | THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA |
DEFSTAN 03-21/3(2002) : 2002 | MECHANICAL METHODS FOR THE INDUCEMENT OF RESIDUAL SURFACE COMPRESSIVE STRESSES |
DEFSTAN 03-14/3(2005) : 2005 | ELECTRO-DEPOSITION OF CHROMIUM FOR ENGINEERING PURPOSES |
DEFSTAN 03-2/4(2005) : 2005 | CLEANING AND PREPARATION OF METAL SURFACES |
BS EN ISO 385:2005 | Laboratory glassware. Burettes |
BS EN ISO 1042:2000 | Laboratory glassware. One-mark volumetric flasks |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.