Steel Hardness conversions
Hardcopy , PDF 1 User , PDF 3 Users , PDF 5 Users , PDF 9 Users
19-02-2019
English, French
01-10-1984
Specifies conversion bands for hardness scales for Vickers/Brinell (steel ball and hardmetal ball), and Vickers/Rockwell (scales A, B, C and D). This conversion bands only apply to non-alloy and low-alloy steels for products of homogeneous structure and of thickness equal to or greater than the figure given in the relevant test standard. In cases of dispute the hardness value obtained from the hardness test should be used. Converted hardness values shall not be used as a basis for rejection of the steel.
DocumentType |
Standard
|
Pages |
7
|
PublisherName |
International Organization for Standardization
|
Status |
Withdrawn
|
Standards | Relationship |
BS 860:1967 | Similar to |
07/30174185 DC : 0 | BS EN ISO 1461 - HOT DIP GALVANIZED COATINGS ON FABRICATED IRON AND STEEL ARTICLES - SPECIFICATIONS AND TEST METHODS |
I.S. EN ISO 14713-2:2009 | ZINC COATINGS - GUIDELINES AND RECOMMENDATIONS FOR THE PROTECTION AGAINST CORROSION OF IRON AND STEEL IN STRUCTURES - PART 2: HOT DIP GALVANIZING |
AWS D3.6M : 2010 | UNDERWATER WELDING CODE |
DIN 50150:2000-10 | TESTING OF METALLIC MATERIALS - CONVERSION OF HARDNESS VALUES |
DIN EN 20898-2:1994-02 | MECHANICAL PROPERTIES OF FASTENERS - PART 2: NUTS WITH COARSE PITCH THREAD AND SPECIFIED PROOF LOAD VALUES |
DIN ISO 14635-2:2010-01 | Gears - FZG test procedures - Part 2: FZG step load test A10/16, 6R/120 for relative scuffing load-carrying capacity of high EP oils (ISO 14635-2:2004) |
DIN ISO 14635-1:2006-05 | Gears - FZG test procedures - Part 1: FZG test method A/8,3/90 for relative scuffing load-carrying capacity of oils (ISO 14635-1:2000) |
ISO 14661:2000 | Thermal turbines for industrial applications (steam turbines, gas expansion turbines) General requirements |
UNI EN ISO 14713-2 : 2010 | ZINC COATINGS - GUIDELINES AND RECOMMENDATIONS FOR THE PROTECTION AGAINST CORROSION OF IRON AND STEEL IN STRUCTURES - PART 2: HOT DIP GALVANIZING |
ISO 683-13:1974 | Heat-treated steels, alloy steels and free-cutting steels Part 13: Wrought stainless steels |
ISO 14635-1:2000 | Gears — FZG test procedures — Part 1: FZG test method A/8,3/90 for relative scuffing load-carrying capacity of oils |
ISO 18265:2013 | Metallic materials — Conversion of hardness values |
BS EN ISO 898-6:1996 | Mechanical properties of fasteners Nuts with specified proof load values. Fine pitch thread |
I.S. EN ISO 18265:2013 | METALLIC MATERIALS - CONVERSION OF HARDNESS VALUES (ISO 18265:2013) |
BS ISO 14635-1:2000 | Gears. FZG test procedures FZG test method A/8, 3/90 for relative scruffing load-carrying capacity of oils |
I.S. EN ISO 898-6:1996 | MECHANICAL PROPERTIES OF FASTENERS - PART 6: NUTS WITH SPECIFIED PROOF LOAD VALUES - FINE PITCH THREAD |
BS EN ISO 14713-2:2009 | Zinc coatings. Guidelines and recommendations for the protection against corrosion of iron and steel in structures Hot dip galvanizing |
11/30210148 DC : 0 | BS EN ISO 18265 - METALLIC MATERIALS - CONVERSION OF HARDNESS VALUES |
BS ISO 14661:2000 | Thermal turbines for industrial applications (steam turbines, gas expansion turbines). General requirements |
UNE-EN ISO 14713-2:2011 | Zinc coatings - Guidelines and recommendations for the protection against corrosion of iron and steel in structures - Part 2: Hot dip galvanizing (ISO 14713-2:2009) |
EN ISO 14713-2:2009 | Zinc coatings - Guidelines and recommendations for the protection against corrosion of iron and steel in structures - Part 2: Hot dip galvanizing (ISO 14713-2:2009) |
DIN EN 623-2:1993-11 | Advanced technical ceramics; monolithic ceramics; general and textural properties; determination of density and porosity |
BS EN 623-2:1993 | Advanced technical ceramics. Monolithic ceramics. General and textural properties. Determination of density and porosity |
UNI EN ISO 18265 : 2014 | METALLIC MATERIALS - CONVERSION OF HARDNESS VALUES |
NF EN ISO 14713-2 : 2010 | ZINC COATINGS - GUIDELINES AND RECOMMENDATIONS FOR THE PROTECTION AGAINST CORROSION OF IRON AND STEEL IN STRUCTURES - PART 2: HOT DIP GALVANIZING |
DIN EN ISO 18265:2014-02 | METALLIC MATERIALS - CONVERSION OF HARDNESS VALUES (ISO 18265:2013) |
ISO 14713-2:2009 | Zinc coatings Guidelines and recommendations for the protection against corrosion of iron and steel in structures Part 2: Hot dip galvanizing |
ISO 14635-2:2004 | Gears — FZG test procedures — Part 2: FZG step load test A10/16, 6R/120 for relative scuffing load-carrying capacity of high EP oils |
BS EN 20898-2:1994 | Mechanical properties of fasteners Nuts with specified proof load values. Coarse thread |
ISO 898-6:1994 | Mechanical properties of fasteners Part 6: Nuts with specified proof load values Fine pitch thread |
UNE-EN ISO 18265:2014 | Metallic materials - Conversion of hardness values (ISO 18265:2013) |
EN 623-2:1993 | Advanced technical ceramics - Monolithic ceramics - General and textural properties - Part 2: Determination of density and porosity |
EN ISO 18265:2013 | Metallic materials - Conversion of hardness values (ISO 18265:2013) |
EN 20898-2 : 1993 | MECHANICAL PROPERTIES OF FASTENERS - PART 2: NUTS WITH SPECIFIED PROOF LOAD VALUES - COARSE THREAD (ISO 898-2:1992) |
EN ISO 898-6:1995 | Mechanical properties of fasteners - Part 6: Nuts with specified proof load values - Fine pitch thread (ISO 898-6:1994) |
DIN ISO 14635-3:2011-08 | Gears - FZG test procedures - Part 3: FZG test method A/2,8/50 for relative scuffing load-carrying capacity and wear characteristics of semifluid gear greases (ISO 14635-3:2005) |
04/30112988 DC : DRAFT APR 2004 | ISO 14635-3 - GEARS - FZG TEST PROCEDURES - FZG TEST METHOD A/2.8/50 FOR RELATIVE SCUFFING LOAD-CARRYING CAPACITY AND WEAR CHARACTERISTICS OF SEMIFLUID GEAR GREASES |
BS EN ISO 18265:2013 | Metallic materials. Conversion of hardness values |
DIN EN ISO 14713-2:2010-05 | ZINC COATINGS - GUIDELINES AND RECOMMENDATIONS FOR THE PROTECTION AGAINST CORROSION OF IRON AND STEEL IN STRUCTURES - PART 2: HOT DIP GALVANIZING |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.