BS L 172:1989
Current
The latest, up-to-date edition.
Specification for extruded, rolled or cast forging stock of aluminium-zinc-magnesium-manganese-copper alloy (for manufacture of forgings to BS L 171) (Zn 5.7, Mg 2.7, Mn 0.5, Cu 0.5) (7014)
Hardcopy , PDF
English
31-01-1990
NO CONTENTS SECTION
Chemical composition, heat treatment, mechanical properties and inspection and testing procedures.
Committee |
ACE/61/-/24
|
DevelopmentNote |
Supersedes 87/75978 DC and 91/73813 DC (08/2005) Reviewed and confirmed by BSI, December 2009. (11/2009)
|
DocumentType |
Standard
|
Pages |
8
|
PublisherName |
British Standards Institution
|
Status |
Current
|
Supersedes |
This British Standard specifies the chemical composition, heat treatment, mechanical properties and the inspection and testing procedures applicable to extruded, rolled, or cast forging stock of aluminium-zinc-magnesium- manganese-copper alloy intended for the manufacture of forgings complying with BS L 171.
BS L 171:1990 | Specification for forging of aluminium-zinc-magnesium-manganese-copper alloy (supplied as-forged or annealed for subsequent heat treatment) (not exceeding 150 mm diameter or minor sectional dimension) (Zn 5.7, Mg 2.7, Mn 0.5, Cu 0.5) (7014) |
BS 5555:1981 | Specification for SI units and recommendations for the use of their multiples and of certain other units |
BS L 171:1990 | Specification for forging of aluminium-zinc-magnesium-manganese-copper alloy (supplied as-forged or annealed for subsequent heat treatment) (not exceeding 150 mm diameter or minor sectional dimension) (Zn 5.7, Mg 2.7, Mn 0.5, Cu 0.5) (7014) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.