Specification for nickel-chromium-titanium heat-resisting alloy cold-worked and softened seamless tubes (nickel base, Cr 19.5, Ti 0.4)
Hardcopy , PDF
31-01-2011
English
30-03-1973
Describes the chemical composition mechanical properties and inspection and test requirements for nickel alloy seamless tubes.
Committee |
ACE/61/-/48
|
DevelopmentNote |
Supersedes 71/39034 DC. (06/2005) Reviewed and confirmed by BSI, December 2009. (11/2009)
|
DocumentType |
Standard
|
Pages |
6
|
PublisherName |
British Standards Institution
|
Status |
Superseded
|
SupersededBy |
BS HR 203:1972 | Specification for nickel-chromium-titanium heat-resisting alloy plate, sheet and strip (nickel base, Cr 19.5, Ti 0.4) |
BS 2HR 504:1973 | Specification for nickel-chromium-titanium heat-resisting alloy bar, wire and rivets (nickel base, Cr 19.5, Ti 0.4) |
BS HR 5:1972 | Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4) |
BS HR 5:1972 | Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4) |
BS 3763:1964 | The International System of units (SI) |
BS 2HR100(1971) : LATEST | |
BS HR 203:1972 | Specification for nickel-chromium-titanium heat-resisting alloy plate, sheet and strip (nickel base, Cr 19.5, Ti 0.4) |
BS 2HR 504:1973 | Specification for nickel-chromium-titanium heat-resisting alloy bar, wire and rivets (nickel base, Cr 19.5, Ti 0.4) |
BS 350:2004 | Conversion factors for units |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.