BS 2TA 24:1973
Withdrawn
A Withdrawn Standard is one, which is removed from sale, and its unique number can no longer be used. The Standard can be withdrawn and not replaced, or it can be withdrawn and replaced by a Standard with a different number.
Specification for forgings of titanium-copper alloy (tensile strength 540-770 N/mm2)
Hardcopy , PDF
25-09-2012
English
30-04-1973
Describes manufacture, inspection and testing of heat resisting alloys for aerospace purposes. Covers forgings, plate, strip, tubes and bars. Gives chemical composition and mechanical properties. Covers forgings of titanium-copper alloy.
Committee |
ACE/61/-/49
|
DevelopmentNote |
Inactive for the new design. Supersedes 72/30563 DC and BS TA24(1968). (11/2003)
|
DocumentType |
Standard
|
Pages |
8
|
PublisherName |
British Standards Institution
|
Status |
Withdrawn
|
BS TA 54:1973 | Specification for forging stock of titanium-copper alloy (tensile strength 650-880 N/mm<sup>2</sup>) (limiting ruling section 75 mm) |
BS 2TA 23:1973 | Specification for forging stock of titanium-copper alloy (tensile strength 540-770 N/mm<sup>2</sup>) |
BS TA 52:1973 | Specification for sheet and strip of titanium-copper alloy (tensile strength 690-920 N/mm<sup>2</sup>) |
BS 2TA 21:1973 | Specification for sheet and strip of titanium-copper alloy (tensile strength 540-700 MPa) |
BS TA 58:1974 | Specification for plate of titanium-copper alloy (tensile strength 520-640 MPa) (maximum thickness 10 mm) |
BS TA 53:1973 | Specification for bar and section for machining of titanium-copper alloy (tensile strength 650-880 N/mm<sup>2</sup>) (limiting ruling section 75 mm) |
BS 2TA 22:1973 | Specification for bar and section for machining of titanium-copper alloy (tensile strength 540-770 N/mm<sup>2</sup>) |
BS TA 55:1973 | Specification for forgings of titanium-copper alloy (tensile strength 650-880 N/mm<sup>2</sup>) (limiting ruling section 75 mm) |
BS TA 55:1973 | Specification for forgings of titanium-copper alloy (tensile strength 650-880 N/mm<sup>2</sup>) (limiting ruling section 75 mm) |
BS 2TA 100:1973 | Procedure for inspection and testing of wrought titanium and titanium alloys |
BS 3763:1976 | The International System of units (SI) |
BS 2TA 22:1973 | Specification for bar and section for machining of titanium-copper alloy (tensile strength 540-770 N/mm<sup>2</sup>) |
BS TA 52:1973 | Specification for sheet and strip of titanium-copper alloy (tensile strength 690-920 N/mm<sup>2</sup>) |
BS 350-2(1962) : LATEST | CONVERSION FACTORS AND TABLES - DETAILED CONVERSION TABLES |
BS TA 53:1973 | Specification for bar and section for machining of titanium-copper alloy (tensile strength 650-880 N/mm<sup>2</sup>) (limiting ruling section 75 mm) |
BS 2TA 21:1973 | Specification for sheet and strip of titanium-copper alloy (tensile strength 540-700 MPa) |
BS TA 54:1973 | Specification for forging stock of titanium-copper alloy (tensile strength 650-880 N/mm<sup>2</sup>) (limiting ruling section 75 mm) |
BS 2TA 23:1973 | Specification for forging stock of titanium-copper alloy (tensile strength 540-770 N/mm<sup>2</sup>) |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.