Standard Specification for Pre-Treatments of Iron or Steel for Reducing Risk of Hydrogen Embrittlement

Available format(s)

Hardcopy , PDF

Superseded date

09-11-2023

Language(s)

English

Published date

01-05-2013

$108.03
Including GST where applicable

CONTAINED IN VOL. 02.05, 2017 Defines procedures for reducing the susceptibility or degree of susceptibility to hydrogen embrittlement or degradation that may arise in electroplating, autocatalytic plating, porcelain enameling, chemical conversion coating, and phosphating and the associated pretreatment processes.

Committee
B 08
DocumentType
Standard
Pages
3
ProductNote
Reconfirmed 2013
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1This specification covers procedures for reducing the susceptibility or degree of susceptibility to hydrogen embrittlement or degradation that may arise in electroplating, autocatalytic plating, porcelain enameling, chemical conversion coating, and phosphating and the associated pretreatment processes. This specification is applicable to those steels whose properties are not affected adversely by baking at 190 to 230°C or higher (see 6.1.1).

1.2The heat treatment procedures established herein have been shown to be effective for reducing the susceptibility of steel parts of tensile strength 1000 MPa or greater that have been machined, ground, cold-formed, or cold-straightened subsequent to heat treatment. This heat-treatment procedure is used prior to any operation capable of hydrogen charging the parts, such as the cleaning procedures prior to electroplating, autocatalytic plating, porcelain enameling, and other chemical coating operations.

Note 11 MPa = 145.1 psi.

1.3This specification has been coordinated with ISO/DIS 9587 and is technically equivalent.

1.4The values stated in SI units are to be regarded as the standard.

ISO 2080:2008 Metallic and other inorganic coatings Surface treatment, metallic and other inorganic coatings Vocabulary
ISO 9587:2007 Metallic and other inorganic coatings Pretreatment of iron or steel to reduce the risk of hydrogen embrittlement
QQ-C-320 Revision B:1974 CHROMIUM PLATING (ELECTRODEPOSITED)

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.

Need help?
Call us on 131 242, then click here to start a Screen Sharing session
so we can help right away! Learn more