ASTM B 456 : 2017 : REDLINE
Current
The latest, up-to-date edition.
Standard Specification for Electrodeposited Coatings of Copper Plus Nickel Plus Chromium and Nickel Plus Chromium
English
03-07-2017
CONTAINED IN VOL. 02.05, 2017 Defines requirements for several types and grades of electrodeposited copper plus nickel plus chromium or nickel plus chromium coatings on steel, nickel plus chromium coatings on copper and copper alloys, nickel plus chromium coatings on Type 300 and 400 series stainless steel and copper plus nickel plus chromium coatings on aluminum and its alloys and zinc alloys for applications where both appearance and protection of the basis metal against corrosion are important.
Committee |
B 08
|
DevelopmentNote |
Supersedes ASTM B 141, ASTM B 142, ASTM B 375 and ASTM B 405 (01/2002) Supersedes ASTM A 166. (04/2002)
|
DocumentType |
Redline
|
Pages |
12
|
PublisherName |
American Society for Testing and Materials
|
Status |
Current
|
1.1This specification covers requirements for several types and grades of electrodeposited copper plus nickel plus chromium or nickel plus chromium coatings on steel, nickel plus chromium coatings on copper and copper alloys, nickel plus chromium coatings on Type 300 and 400 series stainless steel and copper plus nickel plus chromium coatings on aluminum and its alloys and zinc alloys for applications where both appearance and protection of the basis metal against corrosion are important. Five grades of coatings are provided to correspond with the service conditions under which each is expected to provide satisfactory performance: namely, extended very severe, very severe, severe, moderate, and mild. Definitions and typical examples of these service conditions are provided in Appendix X1.
1.2This specification does not cover the requirements for the plating on plastics, see Specification B604.
1.3The following hazards caveat pertains only to the test methods portions, Appendix X2, Appendix X3, Appendix X4, and Appendix X5 of this specification: This standard does not purport to address all of safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
1.4This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
ASTM B 687 : 1999 | Standard Specification for Brass, Copper, and Chromium-Plated Pipe Nipples |
MIL H 22577 : C | HEATING ELEMENTS, ELECTRICAL, CARTRIDGE, SHIP AND TUBULAR TYPE |
ASTM D 4099 : 1995 | Standard Specification for Poly(Vinyl Choride)(PVC) Prime Windows and Sliding Glass Doors (Withdrawn 1999) |
ASTM E 2112 : 2007 : R2016 | Standard Practice for Installation of Exterior Windows, Doors and Skylights |
ASTM B 252 : 1992 : R2004 | Standard Guide for Preparation of Zinc Alloy Die Castings for Electroplating and Conversion Coatings |
ASTM B 252 : 1992 : R2014 | Standard Guide for Preparation of Zinc Alloy Die Castings for Electroplating and Conversion Coatings |
ASTM B 687 : 1999 : R2011 | Standard Specification for Brass, Copper, and Chromium-Plated Pipe Nipples |
MIL-DTL-917 Revision F:2014 | ELECTRIC POWER EQUIPMENT, BASIC REQUIREMENTS FOR |
GG-S-1341 Revision A:1975 | WASHER-STERILIZER, SURGICAL INSTRUMENT |
MIL-STD-1516 Revision B:1990 | UNIFIED CODE FOR COATINGS AND FINISHES FOR DOD MATERIAL |
ASTM B 252 : 1992 : R1998 | Standard Guide for Preparation of Zinc Alloy Die Castings for Electroplating and Conversion Coatings |
ASTM F 737 : 1986 | PERFORMANCE SPECIFICATION FOR ICE HOCKEY SKATE BLADES |
ASTM B 252 : 1992 : R2009 | Standard Guide for Preparation of Zinc Alloy Die Castings for Electroplating and Conversion Coatings |
SAE J 1648 : 2013 | PROTECTIVE COATINGS FOR FASTENERS |
ASTM B 687 : 1999 : R2016 | Standard Specification for Brass, Copper, and Chromium-Plated Pipe Nipples |
ASTM F 1602 : 2012 | Standard Specification for Kettles, Steam-Jacketed, 20 to 200 gal (75.7 to 757 L), Floor or Wall Mounted, Direct Steam, Gas and Electric Heated |
ASTM E 2112 : 2007 | Standard Practice for Installation of Exterior Windows, Doors and Skylights |
I.S. EN ISO 10308:2006 | METALLIC COATINGS - REVIEW OF POROSITY TESTS |
ASTM F 1603 : 2017 : REDLINE | Standard Specification for Kettles, Steam-Jacketed, 32 oz to 20 gal (1 to 75.7 L), Tilting, Table Mounted, Direct Steam, Gas and Electric Heated |
MIL E 917 : E | ELECTRIC POWER EQUIPMENT, BASIC REQUIREMENTS (NAVAL SHIPBOARD USE) |
ASTM B 490 : 2009 : R2014 | Standard Practice for Micrometer Bend Test for Ductility of Electrodeposits |
ASTM B 380 : 1997 : R2008 : EDT 1 | Standard Test Method for Corrosion Testing of Decorative Electrodeposited Coatings by the Corrodkote Procedure |
SAE J 1837 : 2017 | ELECTROPLATE REQUIREMENTS FOR DECORATIVE CHROMIUM DEPOSITS ON ZINC BASE MATERIALS USED FOR EXTERIOR ORNAMENTATION |
ASTM B 764 : 2004 : R2014 | Standard Test Method for Simultaneous Thickness and Electrode Potential Determination of Individual Layers in Multilayer Nickel Deposit (STEP Test) |
ASTM B 490 : 2009 | Standard Practice for Micrometer Bend Test for Ductility of Electrodeposits |
ASTM D 4973 : 1993 | Specification for White Rigid Poly(Vinyl Chloride)(PVC) Insulating Storm Windows (Withdrawn 1999) |
MIL-W-40145 Revision C:1991 | WRENCH, CROWFOOT, SPECIAL |
GG-S-1340 Revision A:1975 | STERILIZER, SURGICAL INSTRUMENT AND SUPPLY GRAVITY AIR REMOVAL, NONPORTABLE (HEAT AND MOISTURE STABLE) |
ASTM B 368 : 2009 | Standard Test Method for Copper-Accelerated Acetic Acid-Salt Spray (Fog) Testing (CASS Test) |
MIL-G-45811 Revision D:1992 | GAGE, AIR, LOW PRESSURE, PNEUMATIC FLOATING EQUIPMENT |
CSA A440.4 : 2007 : R2016 | WINDOW, DOOR, AND SKYLIGHT INSTALLATION |
CSA A440.4 : 2007 | WINDOW, DOOR, AND SKYLIGHT INSTALLATION |
ASTM B 380 : 1997 : R2007 | Standard Test Method of Corrosion Testing of Decorative Electrodeposited Coatings by the Corrodkote Procedure |
ASTM B 380 : 1997 : R2002 | Standard Test Method of Corrosion Testing of Decorative Electrodeposited Coatings by the Corrodkote Procedure |
ASTM E 737 : 1984 : EDT 1 | Practice for Installation of Storm Windows, Replacement Windows, Multi-Glazing, Storm Doors, and Replacement Doors (Withdrawn 1993) |
ASTM F 1602 : 2012 : R2017 | Standard Specification for Kettles, Steam-Jacketed, 20 to 200 gal (75.7 to 757 L), Floor or Wall Mounted, Direct Steam, Gas and Electric Heated |
EN ISO 10308:2006 | Metallic coatings - Review of porosity tests (ISO 10308:2006) |
SAE J 447 : 2016 | PREVENTION OF CORROSION OF MOTOR VEHICLE BODY AND CHASSIS COMPONENTS |
ASTM B 764 : 2004 | Standard Test Method for Simultaneous Thickness and Electrode Potential Determination of Individual Layers in Multilayer Nickel Deposit (STEP Test) |
CSA B125 : 2001 | PLUMBING FITTINGS |
GG-S-1343 Revision A:1975 | STERILIZER, SURGICAL INSTRUMENT AND SUPPLY MECHANICAL AIR REMOVAL, NONPORTABLE (HEAT AND MOISTURE STABLE) |
ASTM B 764 : 2004 : R2009 | Standard Test Method for Simultaneous Thickness and Electrode Potential Determination of Individual Layers in Multilayer Nickel Deposit (STEP Test) |
CSA A440 : 2017 | NORTH AMERICAN FENESTRATION STANDARD/SPECIFICATION FOR WINDOWS, DOORS, AND SKYLIGHTS |
ASTM B 380 : 1997 : R2013 | Standard Test Method for Corrosion Testing of Decorative Electrodeposited Coatings by the Corrodkote Procedure |
ASTM B 368 : 2009 : R2014 | Standard Test Method for Copper-Accelerated Acetic Acid-Salt Spray (Fog) Testing (CASS Test) |
ASTM B 687 : 1999 : R2005 : EDT 1 | Standard Specification for Brass, Copper, and Chromium-Plated Pipe Nipples |
DIN EN ISO 10308:2006-04 | METALLIC COATINGS - REVIEW OF POROSITY TESTS |
BS EN ISO 10308:2006 | Metallic coatings. Review of porosity tests |
ISO 10308:2006 | Metallic coatings Review of porosity tests |
ASTM B 380 : 1997 : R2007 | Standard Test Method of Corrosion Testing of Decorative Electrodeposited Coatings by the Corrodkote Procedure |
ASTM E 50 : 2017 : REDLINE | Standard Practices for Apparatus, Reagents, and Safety Considerations for Chemical Analysis of Metals, Ores, and Related Materials |
ASTM G 85 : 2011 : REDLINE | Standard Practice for Modified Salt Spray (Fog) Testing |
ASTM B 604 : 1991 | SPECIFICATION FOR DECORATIVE ELECTROPLATED COATINGS OF COPPER PLUS NICKEL PLUS CHROMIUM ON PLASTICS |
ISO 1456:2009 | Metallic and other inorganic coatings — Electrodeposited coatings of nickel, nickel plus chromium, copper plus nickel and of copper plus nickel plus chromium |
ASTM B 320 : 1960 : R2019 | Standard Practice for Preparation of Iron Castings for Electroplating |
ASTM B 489 : 1985 : R2018 | Standard Practice for Bend Test for Ductility of Electrodeposited and Autocatalytically Deposited Metal Coatings on Metals |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.