ASTM A 995 : 1998

Withdrawn

Withdrawn

A Withdrawn Standard is one, which is removed from sale, and its unique number can no longer be used. The Standard can be withdrawn and not replaced, or it can be withdrawn and replaced by a Standard with a different number.

View Superseded by

Standard Specification for Castings, Austenitic-Ferritic (Duplex) Stainless Steel, for Pressure-Containing Parts

Available format(s)

Hardcopy , PDF

Withdrawn date

18-02-2021

Superseded by

ASTM A 995/A995M : 2013

Language(s)

English

Published date

31-12-2010

$108.03
Including GST where applicable

CONTAINED IN VOL 01.02, 2002 Covers austenitic-ferritic (duplex) stainless steel castings for valves, fittings, flanges and other pressure-containing parts. The stainless steels give combined enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated Ferrite levels which are not specified, These grades will develop a range of approximately 30 to 60 % ferrite with the balance austenite.

Committee
A 01
DocumentType
Standard
Pages
3
PublisherName
American Society for Testing and Materials
Status
Withdrawn
SupersededBy

1.1 This specification covers austenitic-ferritic (duplex) stainless steel castings for valves, flanges, fittings, and other pressure-containing parts.

1.2 The duplex stainless steels offer a combination of enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated. Ferrite levels are not specified, but these grades will develop a range of approximately 30 to 60 % ferrite with the balance austenite. It is the responsibility of the purchaser to determine which grade shall be furnished depending on design and service conditions, mechanical properties, and corrosion-resistant characteristics.

Note 1 - Because of the possibility of precipitation of embrittling phases, the grades included in this specification are not recommended for service at temperatures above 600 degrees F. (315 degrees C).

1.3 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the specification.

NORSOK M 630 : REV 6 MATERIAL DATA SHEETS AND ELEMENT DATA SHEETS FOR PIPING
API TR 938-C REDLINE : 2011 USE OF DUPLEX STAINLESS STEELS IN THE OIL REFINING INDUSTRY
API TR 938-C : 2015 USE OF DUPLEX STAINLESS STEELS IN THE OIL REFINING INDUSTRY

ASTM E 562 : 2011 : REDLINE Standard Test Method for Determining Volume Fraction by Systematic Manual Point Count
ASTM A 488/A488M : 2017-05 PRACTICE FOR STEEL CASTINGS, WELDING, QUALIFICATIONS OF PROCEDURES AND PERSONNEL
ASTM E 125 : 1963 : R2003 Standard Reference Photographs for Magnetic Particle Indications on Ferrous Castings

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.

Need help?
Call us on 131 242, then click here to start a Screen Sharing session
so we can help right away! Learn more